Welding Engineer Applications Specialist, Heavy Equipment Segment
Our Sites
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Amanda D'Arcy
Hobart Brothers
101 Trade Square East
Troy, OH 45373
937-332-4000
- From The Fabricator
How metal-cored wires reduce hidden welding costs
- By Amanda D'Arcy
- Apr 3, 2012
- Arc Welding
- Article
Metal-cored wire typically costs more than solid wire, but the benefits often offset the per-unit price. In reality, any consumable comprises a relatively small portion of overall welding costs; in fact, material and labor make up the lion’s share of welding expenditures. But in the right application, an increase in filler metal costs may lead to greater savings elsewhere.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
1
Aluminum MIG wires offer smooth feeding, reduced tangling
2
JM Steel triples capacity for solar energy projects at Pennsylvania facility
3
Fabricating favorite childhood memories
4
The role of flux in submerged arc welding performance
5
How laser and TIG welding coexist in the modern job shop
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1
Managing Dangerous Dusts from Metalworking
- June 26, 2024
- Sponsored
- Presented By: Camfil Air Pollution Control