Recent Content on TheFabricator.com for ADMET Inc.

Article
June 13, 2006
Measuring the plastic strain ratio of sheet metals
Determining how much a metal can deform before thinning or fracture occurs is necessary for designing a reproducible forming operation. Testing the incoming sheet material is also essential because material properties may vary from coil to coil and affect the part quality and scrap rate. Understanding a material's plastic strain ratio and how to measure it are crucial in accurately establishing a material's formability.

Products/Services

Material Handling
Clamps and Edge Grabs
Inspection and Testing
Compression Testing Equipment
Inspection and Testing
Tension Testing Equipment