July 11, 2006
Roll forming using spring-loaded top rolls
For certain sheet metal applications, roll forming with spring-loaded top rolls is a practical production method. This article explains the process, describes various machine configurations, and outlines the criteria for suitable applications. It also discusses product requirements that are incompatible with this process.
Article
January 11, 2005
Roll forming basics
Roll forming, often called open-section forming, uses successive sets of roller dies to bend a strip of steel progressively until the desired shape is achieved. This process is very similar to traditional tube- and pipemaking, but differs in that it can form more complicated sections.
Article
September 25, 2003
Roll formers look for a win
Many systems enable users to download a DXF drawing directly into the roll forming line's computer.Not everyone can be the New York Yankees, or even...
Article
May 29, 2003
Roll form tooling tryout and troubleshooting
The secret to developing successful roll tooling—whether for tube production or roll forming—and achieving maximum roll integrity is a simple but often overlooked notion: a comprehensive approach.

Products/Services

Job Shop Services
Machining
Tool and Die
Tube and Pipe Mill Roll Tooling

Related Buyers' Guides

Tooling Buyers' Guide