March 15, 2013
Cryogenic processing—dispelling the myths, mysteries
Heat treating metals goes back thousands of years, but the use of cold temperatures, especially the very cold temperatures in the cryogenic range, is relatively new and hasn't been fully accepted in the manufacturing industry. Interviews with four cryogenic processors clear up some of the mysteries and misconceptions concerning this often-misunderstood process.