Recent Content on TheFabricator.com for Engineering Quality Solutions Inc.

Article
March 8, 2016
Troubleshooting sheet metal defects: Part II
Part II of this series about sheet metal defects focuses on the common problems that can be caused during various stages of the material's production.
Article
July 20, 2015
A closer look at low-carbon sheet steels
Ever wonder what makes up low-carbon steel? Material expert Daniel Schaeffler provides a quick overview.
Article
March 25, 2015
WorldAutoSteel Guidelines for AHSS shed light on lightweighting
Advanced high-strength steels are made differently in the steel mill, and they need to be processed differently in part manufacturing. WorldAutoSteel released forming and welding guidelines intended to help the users of these products work through the differences.
News
January 12, 2010
Web site shares sheet metal product, materials guidance
Engineering Quality Solutions Inc., a technical consulting firm in Southfield, Mich., is providing information to assist Web site visitors with sheet...
Article
July 15, 2008
Forming AHSS: Playing by new rules
Advanced high strength steels spur stampers to think about metal forming in new ways.
Article
September 13, 2005
Introduction to advanced high-strength steels
Part I of this two-part series presented an overview of advanced high-strength steels (AHSS). This article addresses issues encountered when...
Article
September 13, 2005
Introduction to advanced high-strength steels - Part II
Understanding and compensating for the challenges associated with processing advanced high-strength steels (AHSS) can help you minimize springback, edge cracking, trimming, wrinkling, and die wear.
News
September 13, 2005
EQS president elected NADDRG secretary
Engineering Quality Solutions Inc. President Daniel Schaeffler has been elected secretary of the North American Deep Drawing Research Group...
Article
August 9, 2005
Introduction to advanced high-strength steels - Part I
Advanced high-strength steels (AHSS) offer enhanced formability. This article discusses the properties and performance of various grades.

Related Categories

Professional Services
Consulting-Manufacturing Technology
Professional Services
Consulting-Research and Development
Professional Services
Consulting-Value Analysis/Value Engineering
Job Shop Services
Inspection and Testing