Supply chain collaborates on bending project
Faced with a daunting bending contract and a short timeframe, Rick Williams of Rockford Process Control (RPC) sought cooperation from a tubing supplier, bending machine manufacturer, and a tooling supplier at the beginning of the project. The information exchange enabled RPC and its supply chain partners to develop a process, deliver a bender, and engineer and manufacture tooling without the benefit of tubing samples.