A new spin on metal forming
Glenn Metalcraft Inc. started out as a tool and die shop in Minneapolis in 1947. Today it is an $8-million-a-year contract manufacturer that has created a niche in spin-forming circular and conical components up to 0.750 in. thick. Glenn has found a high-volume niche, producing wheels, brakes, and other components, using a process that traditionally was used almost exclusively for prototype and low-volume work.