October 28, 2014
Independence Tube Corporation to open in Alabama
Independence Tube Corporation has announced plans to open in January 2015 in Lawrence County, Ala. The new facility will create 100 manufacturing...
Article
February 1, 2013
Tube producer knocked down, but not out
When one of its facilities was struck by an EF5 tornado on April 27, 2011, Independence Tube Corp. vowed to rebuild the facility. The reconstruction, which was aided by its staff, its customers, and its suppliers, was a Herculean effort that resulted in a small miracle exactly a year later: the new facility reopened for business on April 27, 2012.
News
May 3, 2012
Independence Tube reopens after tornado damage
One year after sustaining major damage from an EF-5 tornado, the Decatur, Ala., location of Independence Tube Corp. has re-opened for business. The...
News
July 13, 2004
Independence Tube announces new manufacturing facility
Independence Tube Corp., a structural tube producer, has announced plans for a new $30 million manufacturing facility to be built on the south bank...

Products/Services

Metals
Tube and Pipe Suppliers

Related Buyers' Guides

Tube & Pipe Supplier Directory