News
March 31, 2015
Ionbond coating center certified to Airbus process specifications
Ionbond has announced that Airbus S.A.S, Blagnac, France, has certified the Greensboro, N.C., coating center for the production of PVD coatings...
News
January 15, 2015
Ionbond demonstration center installs Vapormatt wet blasting machine
Ionbond, a provider of hard, wear-resistant, and low-friction coatings, has installed a Vapormatt Sabre wet blasting machine at its demonstration...
Article
June 28, 2013
An overview of tooling coatings
The ranks within the tool and die community have thinned with the shop closures and business consolidations that followed the Great Recession. As a result, the depth of knowledge about tooling coatings has decreased as well in recent years. This primer is intended to provide a quick explanation of the most common tooling coatings for those that need a quick education.

Products/Services

Job Shop Services
Heat Treating
Tooling Services
Tooling Surface Treatment/Coating

Related Buyers' Guides

Tooling Buyers' Guide