December 7, 2004
Penna Flame Industries increases capabilities
Penna Flame Industries has added induction hardening to its surface hardening capabilities.The company also now offers single-tooth contour gear...
News
November 9, 2004
Penna Flame Ind. Hires induction hardening specialist
Penna Flame Ind. has hired Mark Farley as manager of induction services.Farley has 18 years' experience in induction hardening and contour gear tooth...