April 6, 2004
New bends in the roll
As more commercial buildings are designed with larger open spaces, the beam spans grow longer, and the beams must be bigger and heavier. This requires ever-larger section bending rolls to accommodate this demand. In addition, the trend toward the use of higher strength steels has taxed the capabilities of plate roll bending equipment. These changes and other emerging demands have driven the trend toward the use of CNCs, inline material handling, and larger angle bending rolls.