Prima Power North America Inc.  Arlington Heights, IL

EBe4 .118 S S 88 7.875   S S
EBe5 .125 S S 104 7.875   S S
EBe6 .125 S S 131 7.875   S S
BCe4 .118 S S 88 7.875   S S
BCe5 .125 S S 104 7.875   S S
FBe4 .118 S S 88 7.875   S S
FBe5 .125 S S 104 7.875   S S
FBe6 .125 S S 131 7.875   S S

RAS Systems LLC  Peachtree City, GA

71.30 XLTbend 11 ga. S S 126 25.6 2.75 2.75 120 S S S S S S
71.40 XLTbend 13 ga. S S 159 25.6 2.75 2.75 120 S S S S S S
73.30 FLEXIbend 11 ga. S S 126 11.81 1.57 2.36 90 S S S S S S
73.40 FLEXIbend 13 ga. S S 159 11.81` 1.57 2.36 90 S S S S S S
75.06 XXL Center 16 ga. S S 252 6 2.36 2.36 126 S S S S S S
76.30 GIGAbend .25 S S 126 19.68 2.36 2.36 80 S S S S S S
76.40 GIGAbend .1875 S S 159 19.68 2.36 2.36 80 S S S   S S
78.30 UpDownBend 9 ga. S S 126 23.62 2.95 2.95 110 S S S S S S
78.40 UpDownBend 11 ga. S S 159 23.62 2.95 2.95 110 S S S S S S
78.33 UpDownCenter 11 ga. S S 126 25.5 3.75 3.75 140 S S S S S S
79.05 MiniBendCenter 11 ga. S S 23.6 10 4 4 230 S S S
79.22-2 MultiBend-Center 14 ga. S S 85 16 4 4 290 S S S
79.26-2 MultiBend-Center 14 ga. S S 100 16 4 4 290 S S S
79.30 ProfileCenter 14 ga. S S 126 23.62 3.75 3.75 140 S S S S S S
79.31-2 MultiBend-Center 14 ga. S S 126 16 4 4 290 S S S

Salvagnini America Inc.  Hamilton, OH

P4Xe-2116 .098 S S 98.2 6.50 S   S S
P4Xe-2516 .098 S S 110 6.50 S   S S
P4Xe-2516/3 .126 S S 110 6.50 S   S S
P4Xe-3216 .098 S S 137.6 6.50 S   S S
P4Xe-3216/3 .126 S S 137.6 6.50 S   S S
P4Xe-3816 .098 S S 157 6.50 S   S S
P4Xe-2725 .126 S S 120 10.0 S   S S
P2Xe .098 S S 98.2 6.50 S   S S
P1Xe .048 S S 62.0 5.0 S   S S

Bradbury Group  Moundridge, KS

BCO 18 ga. .042 S S 156 - 480 8 2 2 90 S S S   S
BCO 16 ga. .062 S S 156 - 480 8 2 2 90 S S S   S
BCO 14 ga. .082 S S 252 - 480 8 2 2 90 S S S   S
BCO 11 ga. .125 S S 252 - 480 8 1.5 1.5 60 S S S   S

CIDAN Machinery Inc.  Peachtree City, GA

K15-30 16 ga. S S 122  4.3 2.4 2 90 S S S S S
TH300 Long Folder 11 ga. S S 156 – 480 7.6 1.7 2 50 S S S S
TD150 Double Folder 16 ga. S S 156 – 480 7.6 5.1 5.1 116 S S S S
TD200 Double Folder 14 ga. S S 156 – 480 7.6 5.1 5.1 116 S S S S
TC300 Double Folder 11 ga. S S 252 – 480 7.6 4.7 4.7 100 S S S S
K25-30/K25-40 14 ga. S S 122/159 5.3 1.2 1 75 S S S S S S
Forma 30/40 11/12 ga. S S 122/161 7.6 2.6 2.9 90 S S S S S S
Prolino 25/30/40 7/9/11 ga. S S 102/122/161 7.88 1.36 1.83 75 S S O S S S S
Pro 25/30/40 7/9/11 ga. S S 102/122/161 7.88 1.36 1.83 75 S S S S S S
MegaPro 25/30/40 .315/.250/.197 S S 102/122/161 13.7 1 1.69 50 S S S S S S
TZ125 Long Folder 18 ga. S S 156 – 480 7.6 2.1 2.4 75 S S S S
TZ150 Long Folder 16 ga. S S 156 – 480 7.6 2.1 2.4 75 S S S S
TZ200 LongFolder 14 ga. S S 156 – 480 7.6 2.1 2.4 75 O S S S S

DANOBAT – Sheet Metal Division  Elgoibar (Gipuzkoa), Spain

BM .14 S S 102.36 7.87 S S

Dahlstrom - A Member of the Formtek Group  Warrensville, OH

Custom Wing Benders 12 O O To spec. To spec. To spec. To spec. To spec. O O O O O   O O

Dr. Hochstrate Maschinenbau GmbH  Witten, Germany

2000 1 S S 78 11.8 - 39.37 Var. Var. Var. S S O S S   S S
3000 1 S S 118 11.8 - 39.37 Var. Var. Var. S S O S S   S S
4000 1 S S 157 11.8 - 39.37 Var. Var. Var. S S O S S   S S
5000 .800 S S 196 11.8 - 39.37 Var. Var. Var. S S O S S   S S
6000 .625 S S 236 11.8 - 39.37 Var. Var. Var. S S O S S   S S
8000 .625 S S 315 11.8 - 39.37 Var. Var. Var. S S O S S   S S

Fab-Line Machinery LLC / Baykal  Saint Charles, IL

B12 2160/225/2 .079 S S 85.00 8.85 O O S   S S
B12 2560/225/2 .079 S S 100.78 8.85 O O S   S S
B12 3060/225/2 .079 S S 120.47 8.85 O O S   S S
B12 2560/350/2 .079 S S 100.78 13.78 O O S   S S
B12 3060/350/2 .079 S S 120.47 13.78 O O S   S S
B12 2560/500/2 .079 S S 100.78 19.685 O O S   S S
B12 3060/500/2 .079 S S 120.47 19.685 O O S   S S
B12 4060/225/2 .079 S S 159.84 8.858 O O S   S S
B12 5060/225/2 .079 S S 203.00 8.85 O O S   S S
B12 2160/350/3 .118 S S 85.03 13.78 O O S   S S
B12 2560/350/3 .118 S S 100.787 13.78 O O S   S S
B12 3060/225/3 .118 S S 120.47 8.85 O O S   S S
B12 3060/350/3 .118 S S 120.471 13.78 O O S   S S
B12 4060/300/3 .118 S S 159.84 13.78 O O S   S S

Gigantek SA  Claro, Switzerland

BIMA 3 11 ga. S S 175 7 1.2 2 40 S S S S   S
BIMA 4 11 ga. S S 215 7 1.2 2 40 S S S S   S
BIMA 6 11 ga. S S 295 7 1.2 2 35 S S S S   S
BIMA 8 11 ga. S S 375 7 1.2 2 30 S S S S   S
BIMA 10 11 ga. S S 470 7 1.2 2 30 S S S S   S
BIMA 12 11 ga. S S 550 7 1.2 2 30 S S S S   S

MZM Manufacturing Inc.  Roscoe, IL

 SWF30/48  12 ga. S  30  12  12  12 90  S O O O S S S
 SWF48/60  14 ga. S  48  12  12  12  90 S O O O S S S
 SWF60/60  14 ga. S  60  12  12  12  90 S O O O S S S
 SWF18/36  10 ga. S  18  12  12  12  90 S O O O O O S
 SWF24/36  10 ga. S  24  12  12  12  90 S O O O S S S
 SWF36/48  12 ga. S  36 12   12  12  90 S O O O S S S
 SWF42/60  14 ga. S  42  12  12  12  90 S O O O S S S
 SWF54/60  14 ga. S  54  12  12  12  90 S O O O S S S

MetalForming Inc.  Peachtree City, GA

PowerBend Industrial 40/5 Up/Down 0.196 S S 159 25.6 4.33 4.33 115 S S S S S
PowerBend Professional 20/4 Up/Down 9 ga. S S 80.3 13.77 2.6 2.6 105 S S S S S
Evolution 25/5 Up/Down .196 S S 100 25.6 4.75 4.75 150 S S S S S
PowerBend Professional 25/4 Up/Down 9 ga. S S 100 13.77 2.6 2.6 105 S S S S S
PowerBend Professional 32/3 Up/Down 11 ga. S S 127.5 13.77 2.6 2.6 105 S S S S S
PowerBend Professional 40/2.5 Up/Down .098 S S 159 13.77 2.6 2.6 105 S S S S S
PowerBend Universal 32/3 11 ga. S S 127.5 13.77 1.96 1.96 85 S S S S S
PowerBend Universal 40/2.5 .098 S S 159 13.77 1.96 1.96 85 S S S S S
Evolution 32/4 Up/Down 9 ga. S S 127.5 25.6 4.75 4.75 150 S S S S S
Evolution 40/3 Up/Down 11 ga. S S 159 25.6 4.75 4.75 150 S S S S S
Evolution 32/6 Up/Down .25 S S 127.5 33.5 4.75 4.75 150 S S S S S
Evolution 40/5 Up/Down .196 S S 159 33.5 4.75 4.75 150 S S S S S
Evolution 50/4 Up/Down 9 ga. S S 198 33.5 4.75 4.75 90 S S S S S
PowerBend Industrial 32/6 Up/Down .250 S S 127.5 25.6 4.33 4.33 115 S S S S S

Pivatic Oy  Elgin, IL

FLN Section Bender .049 S S 88 5/4.7 5.1 4.6 110   S S
FLN Section Bender .039 S S 118 5/4.7 5.1 4.6 110   S S
FLN/FSW Panel Bender .049 S S 88 5/4.7 5.1 4.6 110   S S
FLN/FSW Panel Bender .039 S S 118 5/4.7 5.1 4.6 110   S S
FLN/FSW/FSO Casing Bender .039 S S 118 5/80 5.1 4.6 90   S S
FLN300-U Section Bender Heavy Duty .079 S S 118 5/4.7 5.1 4.6 110   S S
FLN300-U/FSW80-U Panel Bender Heavy Duty .079 S S 118 5/4.7 5.1 4.6 110   S S

Roper Whitney  Rockford, IL

AB 1016 16 ga. S S 122 4.5 2.5 2.5 80 S S S   S S
AB 1014 14 ga. S S 122 7.3 2.5 2.5 80 S S S   S S
AB 1014K 14 ga. S S 122 7.3 2.5 2.5 80 S S S   S S
AB 1214 14 ga. S S 147.5 7.3 2.5 2.5 80 S S S   S S
AB 1214K 14 ga. S S 147.5 7.3 2.5 2.5 80 S S S   S S
SBS126-14 14 ga. S S 126 7 2.5 2.5 80 S S S   S O
SBS150-16 16 ga. S S 150 7 2.5 2.5 80 S S S   S O
SBS150-14 14 ga. S S 150 7 2.5 2.5 80 S S S   S O
 AB 1009K  9 ga. S S  126  7.7  3  3  90 O S S O S S S O
Automax 150.64 16 ga. S S 252 7 2.5 2.5 80 S S S S O
 Automax 200.64  14 ga. S S  252  7  2.5  2.5  80 O S S O S S S O
 Automax 300.64  11 ga. S S  252  7  2.5  2.5  80 O S S O S S S O
 Automax 400.64  9 ga. S S  252  7  2.5  2.5  80 O S S O S S S O
 Automax 180  16 ga. S S 252   2.5  2.5  80 O S S O S S S O
 AB 1011K  11 ga. S S  126  7.7  3  3  90 O S S O O S S O

Roto-Die - A Member of the Formtek Group  Warrensville Heights, OH

#5 16 ga. 60 3 S O O  
#10 16 ga. 120 3 S O O  
#15 10 ga. 120 3 S O O  
#15/12 10 ga. 144 3 S O O