Our Sites

AlumaPower 350 MPa

Specifications

Model or Series AlumaPower 350 MPa
Type of Power Source Inverter
Wire Feed Options External
Wire Feed Speed Range
Running Gear Std.
Processes - Brazing
Processes - CAW
Processes - FCAW
Processes - GMAW
Processes - GMAW-P
Processes - GTAW
Processes - GTAW-P
Processes - SAW
Applicable Processes - SMAW
Applicable Processes - Spot
Processes - CAC-A
Processes - Gouging
Output Rating (DC) - Amps 5-425
Output Rating (DC) - Voltage 10-38
Input Rating - Volts (Min.-Max.) 208-575
Input Rating - Phase 1/3
Input Rating - Hz 50/60



Miller Electric Mfg. Co.
1635 W. Spencer St.
P.O. Box 1079
Appleton, WI 54912

Phone: 800-426-4553
Fax: 920-735-4013