5014-ET

Specifications

Model 5014-ET
Operators 1
Punch - U.S. Tons 50
Punch - Std. Dia (in.) 1
Punch - Max Dia. (In.) 2.25
Punch - Throat Depth (In.) 4
Shear - Shear Blade length (in.) 14
Shear - Angle, 90 deg. 4 x 4 x .375
Shear - Angle, 45 deg. 2 x 2 x .375
Shear - Channel
Shear - Flat Bar .5 x 8
Shear - Rod, Round .25-1
Shear - Rod, Square .25-.75
Notcher - Pipe Sch. 40 (in.) .75-2
Notcher - Angle, 90 degree 3 x 3 x .25
Notcher - Rectangle 2.5 x 3 x .3125
Notcher - Vee 6 x 6 x .125
Brake - Rated in U.S. Tons 25
Automatic Positioning Table - S(Standard) O(Optional) N(Not Offered) O
Automatic Positioning Table - X Travel (in.)
Automatic Positioning Table - Y Travel (in.)



Contact Scotchman Industries Inc.

This form is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Scotchman Industries Inc.
180 E. US Hwy. 14
P.O. Box 850
Philip, SD 57567

Phone: 605-859-2542
Fax: 605-859-2499

scotchman.com

Sales Contact
Jerry Kroetch - President
jerrykroetch@scotchman.com
605-859-2542