Spectrum 625 X-TREME
Specifications
Model or Series | Spectrum 625 X-TREME |
Input – Volts | 120/240 |
Input – Single-phase | |
Input – 3 Phase | |
Input – 50 Hertz | |
Input – 60 Hertz | |
Output – Volts | 140 |
Output – Current (Amps) | 40 |
Output – Kilowatts | 6.5 |
Duty Cycle - Percent | 60 |
Duty Cycle - Temperature (C) | 40 |
Capacity in Mild Steel – Max. Cutting Thickness (In.) | .625 |
Capacity in Mild Steel – Max. Cutting Speed at Max. Thickness (IPM) | 13 |
Capacity in Mild Steel – Recommeded Cutting Thickness | |
Capacity in Mild Steel – Recommended Piercing Thickness | .3125 |
Capacity in Mild Steel – Recommended Severing Thickness | .875 |
Air Pressure Required (PSI) | 90 |
Airflow Required (CFM) | 6 |
Arc Start - Standard Frequency | |
Arc Start - High Frequency | |
Weight (lbs.) | 21 |
Miller Electric Mfg. Co.
1635 W. Spencer St.
P.O. Box 1079
Appleton, WI 54912
Phone: 800-426-4553
Fax: 920-735-4013
MillerWelds.com
1635 W. Spencer St.
P.O. Box 1079
Appleton, WI 54912
Phone: 800-426-4553
Fax: 920-735-4013
MillerWelds.com