AirCut15C
Specifications
Model or Series | AirCut15C |
Input – Volts | 120 |
Input – Single-phase | |
Input – 3 Phase | |
Input – 50 Hertz | |
Input – 60 Hertz | |
Output – Volts | |
Output – Current (Amps) | 15 |
Output – Kilowatts | |
Duty Cycle - Percent | 35 |
Duty Cycle - Temperature (C) | |
Capacity in Mild Steel – Max. Cutting Thickness (In.) | .1875 |
Capacity in Mild Steel – Max. Cutting Speed at Max. Thickness (IPM) | 20 |
Capacity in Mild Steel – Recommeded Cutting Thickness | .125 |
Capacity in Mild Steel – Recommended Piercing Thickness | .1875 |
Capacity in Mild Steel – Recommended Severing Thickness | .1875 |
Air Pressure Required (PSI) | |
Airflow Required (CFM) | |
Arc Start - Standard Frequency | |
Arc Start - High Frequency | |
Weight (lbs.) | 29 |
Thermal Dynamics
82 Benning St.
West Lebanon, NH 03784
Phone: 866-279-2628
Fax: 248-553-6841
thermal-dynamics.com
82 Benning St.
West Lebanon, NH 03784
Phone: 866-279-2628
Fax: 248-553-6841