Plate Rolling Machine Buyers' Guide



Machine Type and Features Roll
Positioning
and Drive
System
Material Options
Model Series

JMT USA  Salt Lake City, UT

JMT HRB-C Custom Series 2-40 6 - 60 NC, CNC .1 - 6 39 - 170
JMT HRB-4 Roll with Dynamic Crowning (Manual or CNC) 2-40 5.51 - 60 PLC, NC, CNC .075 - 6.375 39 - 170
JMT HRB-4 4000 Series (Hydraulic 4-Roll) 13 10.63 - 20.47 PLC, NC, CNC .156 - 1.375 39 - 170
JMT HRB-4 3000 Series (Hydraulic 4-Roll) 10 8.27 - 42.13 PLC, NC, CNC .156 - 6.375 39 - 170
JMT HRB-4 2500 Series (Hydraulic 4-Roll) 8 7.87 - 20.47 PLC, NC, CNC .156 - 2.5 39 - 170
JMT HRB-4 2000 Series (Hydraulic, 4-Roll) 6 5.51 - 19.29 PLC, NC, CNC .075 - 2.5 39 - 170
JMT HRB-4 1500 Series (Hydraulic, 4-Roll) 5 5.51 - 6.69 PLC, NC, CNC .125 - .3125 39 - 170
JMT HRB-3V 4000 Series (Variable Geometry, 3-Roll) 13 15 - 20 PLC, NC .44 - 1.57 39 - 170
JMT HRB-3V 3000 Series (Variable Geometry, 3-Roll) 10 15.75 - 40.12 PLC, NC 1 - 6.5 39 - 170
JMT MRB Series (Mechanical Slip Rolls) 3-10 2.2 - 8.66 DRO .048 - .3125 39
JMT HRB-3 4000 Series (Hydraulic, 3-Roll) 13 10.63 - 20.47 PLC, NC, CNC .156 - 1.375 39 - 170
JMT HRB-3 3000 Series (Hydraulic, 3-Roll) 10 8.66 - 20.47 PLC, NC, CNC .156 - 2 39 - 170
JMT HRB-3 2500 Series (Hydraulic, 3- Roll) 8 7.87 - 17.72 PLC, NC, CNC .156 - 1.56 39 - 170
JMT HRB-3 2000 Series (Hydraulic, 3- Roll) 6 7.28 - 17.72 PLC, NC, CNC .156 - 2 39 - 170

Trilogy Machinery Inc.  Belcamp, MD

Refurbished Roundo Rolls 3 - 32 4.3 - 40 CNC 10 ga. - 8 in. 42
 SWEBEND PB3 - 3 Roll Double-Pinch  3-32  4.3-40  NC  10 ga.- 8 in.  42
 SWEBEND PB4 - 4 Roll  3-32  4-40  CNC  10 ga.- 8 in. 42
LEMAS - 4 Roll 4 -1 0 3.14 - 7.87 NC .063 - .500 38
LEMAS - 3 Roll 3 - 10 3.14 - 7.87 .063 - .500 38
AKYAPAK AkBend AHS 4-Roll 4 - 30 6 - 40 NC, CNC Gauge - 6 in. 38
AKYAPAK AkBend AHK 3-Roll 4 - 30 6 - 40 NC, CNC Gauge - 6 in. 38
AKYAPAK AkBend AHV 3-Roll Var. Geometry 4 - 30 6 - 40 NC, CNC .5 - 6 38

1960 Seravesi Srl  Pallazzolo Sull'Olio (BS), Italy

           
 E79-S Series 6 - 20 40 - 60  NC 6 - 16 150
RI 72 Series 2 - 20 12 - 60 NC, CNC .500 - 12 150
RI 72-3 Series 2 - 20 12 - 40 .250 - 2 150
E79 Series 2 - 20 15 - 40 NC 1 - 6 150

Bertsch - A Division of MegaFab  Rockford, IL

3IP 1 - 40 9 - 40 DRO .25 - 4 50
4R 1 - 40 9 - 40 NC/CNC .25 - 4 50
M-Series 2 - 10 4.7 -14.8 DRO 20 ga. -.75 50

C. Marshall Fabrication Machinery Inc.  Peoria, AZ

M3015C 10 11.4 Opt. CNC EVO Touch Command, NEXUS Touch Screen .562 38.5
M3022D 10 13.8 Opt. CNC EVO Touch Command, NEXUS Touch Screen .875 38.5
 M3028M  10  15  Opt. CNC EVO Touch Command, NEXUS Touch Screen Control  1.125  36.8
 G3014C  10  11.4 .5625  38.5
 G3022D  10  13.8  .875  38.5
 M3048G  10  18.9   Opt. CNC EVO Touch Command, NEXUS Touch Screen  1.89  38.5
 M3048G  10  18.9  Opt. CNC EVO Touch Command, NEXUS Touch Screen  1.89  38.5
 M2006P  6.7  7.1   Opt. CNC EVO Touch Command, NEXUS Touch Screen  .250  38.5
M0501L  1.75  2.8   Opt. CNC EVO Touch Command, NEXUS Touch Screen  .064  38.5
 F05A  21  3.1    .047  38.5
 F20B  81  6.3   .16  38.5
 PH26.320  114  17.7    2.2  38.5
 PH3.500  10  20    2.375  38.5
 PH3.1500  10  32.3    5.1  38.5
 G6032H  20  22.8   Opt. CNC EVO Touch Command, NEXUS Touch Screen  1.250  38.5

CO.MA.L - JD FORMAT HOLDING  Trezzo Sull'adda, Milan Italy

  1.64 - 13.5 2.36 - 21.65 NC, CNC  14ga - 2.56 50

COLE-TUVE Inc  White Marsh, MD

 IR  3 - 6  1.81 - 2.95    22 ga. - 14 ga.  
MSM 3 - 6 3.54 - 3.94 16 ga. - 10 ga.
IRM 3 - 8 4.33 - 5.51 14 ga. - .1875
MRMS 3 - 10 5.12 - 8.66 11 ga. - .375
MRMH 2 - 13 3.15- 9.84 16 ga. - .563
3R HS, 3R HSS 6 - 13 8.27 - 21.66 .250 - 2.156
3R UHS 8 - 13 17.72 - 26.77 NC 1.50 - 4
4R HMS 2 - 13 2.36 - 9.84 NC 25 ga. - .375
4R HS, 4R HSS 3 - 13 5.91 - 26.77 NC, CNC .250 - 2.750

COMEQ Inc.  White Marsh, MD

Parmigiani Model TBH Hydrotronic 1.5 - 26 6 - 63 CNC, NC .25 - 16 65
Parmigiani Model VBH Hydrotronic 1.5 - 26 6 - 63 CNC, NC .25 - 16 65
Americor Model 3RSP 2 - 10 3.15 - 9.84 NC 16 ga. - .562 52
Americor Model 4RDP 2 - 10 3.15 - 9.84 NC 16 ga. - .562 52
Parmigiani Model PCO 3 - 26 10 - 63 NC, Manual, CNC .25 - 12 58
Parmigiani Model HDC 1 - 50 6 - 12 CNC, NC .03 - .75 50
Custom Models To Spec. 3 to 50 To Spec. To Spec. To Spec.

Carell Corp.  Stapleton, AL

4RH 6 - 12 8.7 - 14.2 NC, CNC .156 - 1 36 - 50
4RH PBS 6 - 12 15.4 - 25.6 NC, CNC .625 - 3.25 36 - 50
4RH 100 3 - 10 6.7 NC, CNC 12 ga. - .25 36 - 50
SIHR 6.72 - 13.28 7.8 - 13 NC, CNC .156 - 1 36 - 50
SIH-PBS 6 - 12 13.78 - 25.6 NC .625 - 3.5 36 - 50
3RHT 6 - 16 15 - 32 NC .625 - 4.50 36 - 50
HI-TECH HTH 3.1 - 6 5.1 - 6.7 NC, CNC 16 ga. - .1875 35 - 50
HI-TECH HT 1.6 - 5 2.36 - 4.17 NC, CNC .017 - .089 36 - 50
HI-TECH 2R 2 - 5 3 - 5 NC .02 - .12 36 - 50
A31 3 - 10 4.5 - 7.9 NC .074 - .281 36 - 50
Q41 3 - 10 4.33 - 7.48 NC, CNC 20 ga. - .3125 36 - 50
LS 3 - 6 2.4 - 4.5 NC 20 ga. - 12 ga. 36 - 50

Davi Inc.  Dallas, TX

MCP 4 - 20 4 - 60 CNC .25 - 16 62
MCO 4 - 30 4 - 60 CNC .25 - 16 62
MAV 4 - 40 10 - 60 CNC .75 - 16 62
MCA - MCB 4 - 40 4 - 60 CNC .25 - 16 62
AER 4 - 40 2 - 20 CNC 12 ga. - 1 62

Durma  Cornelius, NC

MS 3 - 10 2.2 - 8.6  DRO .040 - .314 35
HRB-3 6 - 10 7.2 - 15.7 DRO .25 - 1 35
 HRB-4 5 - 26  5.5 - 30 NC, CNC .157 - 4.7 35
 HRB-4DC-Dynamic Crowning 6 - 10 6 - 10 CNC .25 - .75 35
 HRB-3V  10 & 13 14 x 40  PLC-NC  .44 - 6.5  35

E.G. Heller's Son, INC  Los Angeles, CA

   2-26 2-30  NC, CNC, MultiaxisTouch Command  16 ga.-8 40

Fabrication Solutions & Technologies, an IMCAR Company  Judson, TX

 4R 6 - 20 * 6.7 - 17 * Standard .188 - 1.75 36 - 50
4RH 6 - 20 * 8.6 - 23.6 *  NC, CNC .188 - 4 36 - 50
3RHT 6 - 20 * 15 - 32 *  NC, CNC .75 - 5 36 - 50
SIHR 6 - 20 * 7.8 - 13  NC, CNC .125 - 1 36 - 50
SIH 6 - 20 * 13 - 26  NC, CNC .500 - 4 (or To Spec.) 36 - 50
Hi-Tech HTH 1.5 - 6.5 5 - 7  NC, CNC 16 ga. - .188 36 - 50
Hi-Tech HTP Pneumatic 1.5 - 6.5 2.3 - 5  NC, CNC 12 ga. - 24 ga. 36 - 50
Hi-Tech HT2 2 Roll 1.5 - 6.5 3 - 5  NC, CNC 24 ga. - .125 36 - 50
View Details * Can be made to spec. * Can be made to spec.

Faccin  Visano, Italy

HCU Series 2 - 8 2.50 - 15 NC / CNC .030 - .197 52
ASI Series 3 - 10 5 - 6.75 DRO .059 - .354 52
DP3/3HEL Series 5 - 13 6 - 13.375 DRO .118 - .984 52
HAV Series 6 - 60 13.375 - 52 PLC .591 - 17 52
4HEL Series 2 - 40 5 - 48 NC / CNC .098 - 8 52
Specialty 10 - 70 To Spec. NC / CNC .032 - 6 52
Biko B3 Series 5 - 20 6 - 38 DRO .236 - 5 52
Biko B4 Series 5 - 20 6 - 38 NC / CNC .079 - 5 52

GV Fabricating Machinery Sales  Naples, FL

           
BTR 3-5 5-5.5 Manual, NC 16-12 ga. 36
CY 3-5 2.7-3.7 Manual 24-12 ga. 36
CLY 3-10 4.3-5.5 Manual 12 ga.-.1875 36
CLY-ST 3-10 5.5-8 Manual 10 ga.-.3125 36
CYL-STH 3-10 5.5-10.5 Manual 10 ga.-.50 36
BHK 3-20 5.5 - 24 Manual, NC 10 ga.-2 36
BHS 3-20 5.5 - 24 Manual, NC, CNC 10 ga.-2 36

HAEUSLER  Duggingen, Switzerland

SPBM 20-80 10-25 NC, CNC .5-2.0 70
FKB 10 - 40 .75 - 6 NC, CNC .02 - .6 52
Rollmeister TETRA 6-14 10-20.5 CNC .2-1.5 37
VRM 1 - 30 10 - 65 NC, CNC .25 - 16 70
HDR 1 - 30 15 - 65 NC, CNC 1 - 16 70
RMaut .1 - 6 .75 - 20 CNC .04 - 1.0 70
RMS 20 - 43 7.8 - 38 CNC .25 - 1.65 87
 HHT  30 - 80  7.8 - 38  CNC .25 - 2.0  87

Ilvita  Siauliai, Lithuania

           

KAAST Machine Tools, Inc.  Ardmore, PA

RB 3 - 6 2.1 - 3.7 .036 - .1345 36
RDB-3M 3 - 6 3 - 4 DRO 20 ga. - 11 ga. 36
RBD-3M 3 - 7 4 - 5.5 DRO 14 ga. - .2 in. 36
RBD-3M 3 - 10 5 - 8 DRO .188 - .375 36
RBD-3HL 6 - 14 8.5 - 12 NC .25 - .625 36
RBD-3HD 6 - 14 12 - 18 NC .5 - 1.5 36
RBD-4HD 3 - 14 6 - 21 CNC .5 - 2.25 36
RBD-4MAX 6 - 20 11 - 32 CNC .75 - 8 36

KNUTH Machine Tools USA Inc.  Lincolnshire, IL

KRM-A 3.4 - 6.66 3.5 - 3.75 NC .08 - .13
KRM 3.4 - 6.75 4.25 - 5.5 NC .14 - .22
KRM-S 5.25 - 10.16 6.75 - 7.5 NC .16 - .31
RBM 6.83 - 13.42 6.3 - 25.3 CNC .236 - 1.17

MG S.r.l.  Fossano, Cuneo Italy

PH - 3 rolls 3.44 - 15 14 - 60 CNC .8 - 14 36
G 3 rolls 1.15 - 26 1.9 - 60 NC .0135 - 12 36
M 4 rolls 1.15 - 26 1.9 - 60 CNC, NC .031 - 12 36
F 2 - 7 NC, CNC Up to .118 36

Marando industries, Inc.  Reading , PA

Roll Bender 12-42 15-40 CNC .5-6 180

Parmigiani  Cremona, Italy

HDC Aircraft 6 - 30 1 - 8 CNC .02 - 1.00 80
HDC Shipbuliding 20 - 60 8 - 30 CNC .25 - 4 60
VBH 4-roll 3 - 36 1 - 70 CNC .1 - 10 60
PCO 3-roll variable axis 1.5 - 27 5 - 70 NC, CNC .5 - 10 60
TBH 3-roll pyramid type 2 - 20 5 - 45 NC .2 - 6 60

Quantum Machinery Group  Mira Loma, CA

HR4W1206 4 4.72 NC, CNC .23 37.7
HR4W2015 6.5 9.8 NC, CNC .59 37.7
HR4W2515 8.5 10.63 NC, CNC .59 37.7
HR4W3008 10 9.05 NC, CNC .315 37.7
HR4W4006 13 9.6 NC, CNC .23 37.7
HR4W6008 20 13.78 NC, CNC .315 37.7
HR3W2020 6.5 10.63 NC, CNC .78 37.7
HR3W2550 8.5 17.71 NC, CNC 1.9 37.7
HR3W4032 13 20 NC, CNC 1.26 37.7
HR4W2020 6.5 11 NC, CNC .78 37.7
HR4W4025 13 18 NC, CNC .98 37.7
HR4W5032 16.5 22 NC, CNC .98 37.7
HR4W30150 10 40.94 NC, CNC 5.90 37.7
HR4W6060 20 32.28 NC, CNC 2.36 37.7
HR3W6040 20 28.34 NC, CNC 1.57 37.7

Rishbin  Wuxi, Jiangsu China

           

Sahinler Metal Makina  Bursa, Turkey

4R HSS 25 Series 8.25 11 - 21.65 NC or CNC 37.7
4R HSS 30 Series 10 11 - 21.65 NC or CNC 37.7
4R HSS 40 Series 13.45 11 - 21.65 NC or CNC 37.7
4R HSS 60 Series 20 11 - 21.65 NC or CNC 37.7
4R HSS 20 Series 6.73 11 - 21.65 NC or CNC 37.7

Westway Machinery  Mississauga, ON Canada

4R HS 15-170 5 6.5 .25 36
4R HS 25-220 8 8.5 .25 36
4R HS 30-245 10 9.5 .25 36
4R HSS 30-280 10 11 .50 36
4R HSS 30-320 10 12.5 .625 36
4R HSS 30-400 10 16 1 36
4R HSS 30-620 10 24 2 36
MRM-440 4 4.25 .157 36
MRM-555 5 5.5 .194 36
MRM-655 6 5.5 .194 36
MRM-640 6 4.25 .105 36
MRMS-880 8 7.874 .281 36
4R HMS 5 7 .25 36