Our Sites

Euromaster 45-75

Specifications

Series Euromaster 45-75
Type (E, EH,EHP, EM, H, HM, M, P, PM) EHP
Upstroking
Downstroking
Length (in.) - Overall 63-122
Length - Between Housings 43-82
Maximum Tonnage 75
Shut Height (in.) 7.1
Stroke Length (in.) 3.9
Open Height (in.) 11
Throat Depth (in.) 7.8
Maximum Postitioning Speed (IPM) - Rapid Approach 189
Maximum Speed - Press Speed 24
Maximum Speed - Return Speed 165
Gauges - Front
Gauges - Back
Offline Programming
Light Curtain
Network Capable

E-Electric, EH-Electric Hydraulic, EHP-Electronic-Hydraulic Position, EM-Electric Mechanical, H-Hydraulic, M-Mechanical, P-Pneumatic, PM-Pneumatic Mechanical



Haco-Atlantic Inc.
11629 N. Houston Rosslyn Road
Houston, TX 77086

Phone: 281-445-3985
Fax: 281-445-3989

hacoatlantic.com

Sales Contact
Daniel Kint - Sales Manager
Sales.Tx@HacoAtlantic.com
281-445-3985