APHS 6000
Specifications
Series | APHS 6000 |
Type (E, EH,EHP, EM, H, HM, M, P, PM) | H |
Upstroking | |
Downstroking | |
Length (in.) - Overall | 360 |
Length - Between Housings | 312 |
Maximum Tonnage | 6,600 |
Shut Height (in.) | 52 |
Stroke Length (in.) | 48 |
Open Height (in.) | 100 |
Throat Depth (in.) | 60 |
Maximum Postitioning Speed (IPM) - Rapid Approach | 118 |
Maximum Speed - Press Speed | 9 |
Maximum Speed - Return Speed | 94 |
Gauges - Front | |
Gauges - Back | |
Offline Programming | |
Light Curtain | |
Network Capable |
E-Electric, EH-Electric Hydraulic, EHP-Electronic-Hydraulic Position, EM-Electric Mechanical, H-Hydraulic, M-Mechanical, P-Pneumatic, PM-Pneumatic Mechanical
Fab-Line Machinery LLC / Baykal
P.O. Box 308
Saint Charles, IL 60175
Phone: 630-587-0505
Fax: 630-587-5584
fab-line.com
pcanning@fab-line.com
630-587-0505
866-466-8298
P.O. Box 308
Saint Charles, IL 60175
Phone: 630-587-0505
Fax: 630-587-5584
fab-line.com
Sales Contact
Patrick Canning - Presidentpcanning@fab-line.com
630-587-0505
866-466-8298