Robotic Welding Workcell Buyers' Guide



Workcell Robot(s)
Robot
Reach
Positioner Type* No. of
Axes
Positioner
Load
Capacity
per Side
Workcell
Footprint
Welding Process PC Based Software Maximum
Part/Tool Size
Robot External GMAW GTAW Laser Spot Plasma FCAW

ABB Inc.  Auburn Hills, MI

ArcPack Lean 1410 IRB 1410 .057 To spec. 6 Up to 3 To spec.
FlexArc 500C Single IRB 1600 .047-.057 IRBP 500C 6 3 500 17.4 x 11.8 x 8.2
FlexArc 500C Multimove IRB 1600 (2) .047-.057 IRBP 500C 6 3 1,102 17.4 x 11.8 x 8.2
FlexArc 250R Single IRB 1600 .047-.057 IRBP 250R 6 3 551 17.4 x 11.8 x 8.2
FlexArc 250R Multimove IRB 1600 (2) .047-.057 IRBP 250R 6 3 551 17.4 x 11.8 x 8.2
FlexArc 500R Single IRB 1600 .047-.057 IRBP 500R 6 3 1,102 22 x 12.1 x 8.2
FlexArc 750R Single IRB 1600 .047-.057 IRBP 750R 6 3 1,653 22 x 12.1 x 8.2
FlexArc 250K Single IRB 1600 .047-.057 IRBP 250K 6 3 551 18 x 14.1 x 8.2
FlexArc 500K Single IRB 1600 .047-.057 IRBP 500K 6 3 1,102 19.7 x 17.4 x 9.8
FlexArc 750K Single IRB 1600 .047-.057 IRBP 750K 6 3 1,653 19.7 x 17.4 x 9.8

TRUMPF Inc.  Farmington, CT

TruLaser Cell 7040 TRUMPF Multiaxis 160 x 60(80) x 30 To spec. 5 1 1,764
TruLaser Cell 7020 TRUMPF Multiaxis 80 x 60(80) x 30 To spec. 5 1 1,764
TruLaser Cell 7006 Powertrain TRUMPF Multiaxis 26 x 80 x 30 To spec. 5 1 To spec. 240 x 282 x 150 To spec.
TruLaserCell 1100 TRUMPF Multiaxis 11.8 x 11.8 To spec. 2 2 To spec. 250 x 155 x 107.5
TruLaser Cell 3000 TRUMPF Multiaxis 31, 24, 16 5 209.4 62.4 x 111.6 x 104.4
TruLaser Robot 5020 KUKA KRC4 80 To spec. 6 To spec. 551 352x230 (with resonator, chiller) To spec.

FANUC America Corporation  Rochester Hills, MI

ARC Mate 50iC/5L ARC Mate 50iC/5L 35.1 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC/10S ARC Mate 100iC/10S 43.2 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC ARC Mate 100iC 55.9 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iC/6L ARC Mate 100iC/6L 63.8 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 120iC ARC Mate 120iC 71.3 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 120iC/10L ARC Mate 120iC/10L 79.1 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.
ARC Mate 100iCe ARC Mate 100iCe 55.9 Fixed T To spec. To spec. To spec.
M710iC/20L-SA M710iC/20L-SA 122.4 HS, 2-axis positioner; to spec. Multiple Multiple 1,102/2,205/3,307 To spec. To spec.

Liburdi Automation Inc.  Dundas, ON Canada

LAWS 445, 645, 800, 1000 FANUC 24 x 36 x 18 Vision-based compensation (+/-.002) 6 Up to 10 Var. 4 x 4 x 7 2 x 2 - 3 x 4

Lincoln Electric Co., The  Cleveland, OH

Robotic Welding Education Cell FANUC ARC Mate® 50iD/7L 35.11 6 81 x 64 x 66 (sides expanded)
System 5 FANUC ARC Mate 100iC 55.9 6 2,500 69 x 123 24 x 70
System 10 FANUC ARC Mate 100iC 55.9 6 2,500 69 x 127 (2) 37x35
System 15 FANUC ARC Mate 50iC/5L 35.11 6 400 62.5 x 89 52
System 20 FANUC ARC Mate 100iC 55.9 6 600 126 x 84 58
System 30 FANUC ARC Mate 100iC 55.9 6 2,500 80 x 181 (2) 36x42
System 35 FANUC ARC Mate 100iC 55.9 6 2,500 154 x 137 (2) 78x39
System 30HS FANUC ARC Mate 100iC 55.9 6 2,000 - 6,000 80 x 181 30 x 30
System 40 FANUC ARC Mate 100iC 55.9 6 800 86 x 148.5 76
System 50HP FANUC ARC Mate 100iC 55.9 6 2,000-6,000 82 x 188 40 x 54
System 55 FANUC ARC Mate iC Family To spec. As needed 6 2,000-6,000 To spec. 36-72 x 84-144

Motoman Inc.  Miamisburg, OH

ArcWorld C/ArcWorld II-50 Series MA1400, VA1400 F, RT 6, 7 1 or 2 396 21.65 x 27.55, 51.18 x 27.55 dia.
ArcWorld II-200/500 Series MA1400, VA1400 F, RT 6, 7 1 or 2 1,212 39.37 x 31.49 dia.
AWC-500 Series MA1400, VA1400 F, RT, T/R 6, 7 2 or 4 2,369 51.18 x 43.30 dia
Arcworld 1000 MA1400, VA1400 TT 6, 7, 12, 14 0 661, 1,102 39.37 x 25.59
ArcWorld IV-4000 MA1400, MA1900 TT, RT 6, 12 3 1,102, 1,653 78.74 x 51.18 dia.
ArcWorld IV-6000SL MA1400, VA1400, MA1900 FW 6, 12, 18, 24; 7, 14, 21 3 551, 1,653 78.74, 118.11 x 51.18 dia.
ArcWorld IV-6000XHD MA1400, VA1400, MA1900 FW 6, 12, 18, 24; 7, 14, 21 3 2,645 118.11 x 51.18 dia.
ArcWorld V-6000 MA1400, VA1400, MA1900 FW 6, 12, 18, 24; 7, 14, 21 3 2,645 118.11 x 51.18 dia.
FabWorld, FabWorld II MA1900 (1 or 2); MA3100 74.80, 122.04 RT 6, 12 2 2,369, 6,613, 13,888 118.11 x 51.18, 157.48 x 78.74 dia.

OTC Daihen Inc.  Tipp City, OH

ECO-ARC 200 FD-V6, FD-B4 55 2 static tables 6 0 550 86.4 x 84.6 x 135 31.5 x 23.6/side
ECO-ARC 200L FD-V6L, FD-B4L 79 2 static tables 6 0 550 133.6 x 84.6 x 160 48 x 36/side
PT-ARC 600 FD-V6, FD-B4 55 60 pneumatic TT 6 0 550 86.4 x 88.0 x 180.5 60 x 30
SERVO-ARC 600 FD-V6, FD-B4 55 60 servo TT 6 1 550 86.4 x 88.0 x 180.5 60 x 30
SERVO-ARC 720 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 72 servo TT 6 1 550 86.4 x 88.0 x 180.5 72 x 36
ROTA-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing H frame 6 3 2,200 133.8 x 86.6 x 240.7 59.06 x 39.37
TRI-ARC 500 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing FW 6 3 1,100 246.4 x 120 x 225.8 137.79 x 41.34
TRI-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS indexing FW 6 3 2,200 246.4 x 120 x 225.8 137.79 x 41.34
DT-ARC 500 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS/TS 6 2 1,100 165 x 93 x 227 78.7 x 39.37
DT-ARC 1000 FD-V6, FD-B4, FD-V6L, FD-B4L 55, 79 Dual servo HS/TS 6 2 2,200 165 x 93 x 227 78.7 x 39.37

Taylor-Winfield Technologies  Youngstown, OH

Custom To spec. To spec. To spec. To spec. To spec. To spec. To spec. To spec.

Westwood Manufacturing Inc.  Elizabethtown, NC

Auto-Shuttle/Auto Table/Flex ARCS ABB/Kuka 118 Servo positioners 6 7 165 Various Various

Worker Automation Inc.  Covington, OH

ePRO® II Dual Table OTC 55, 79 Stationary T 6 0 1,000 7.3 x 11.1 32 x 40
ARCWORKER® ET-60, 72, 84 OTC 55, 79 TT 6 0 500 - 1,000 7.5 x 15 29 x 32
ARCWORKER® 2H OTC 55, 79 2 HS/TS 6 2 500 - 5,500 15 x 15.5 86 x 192
ARCWORKER® 3S OTC 55, 79 2 HS/TS on TT 6 3 500 - 4,000 7.6 x 10 60 x 88
ARCWORKER® Dual TR OTC 55, 79 Tilt & Rotate 6 4 660 - 8,000 7.6 x 14.8 48 x 48
LASERWORKER® OTC 55+ Many 6 0 To spec. To spec. To spec.
ARCWORKER® 5S OTC 55, 79 5-axis 6 5 500 - 2,500 13 x 18 60 x 80
ARCWORKER® FW OTC 55, 79 FW 6 3 500 - 4,000 10 x 12 52 x 144
ARCWORKER® Dual Robots (opt.) OTC 55, 79 TT 6 0 500-4,000/750-4,000 To spec. To spec.
Swing Arm & Gantry OTC 55, 79 To spec. 6 4 To spec. To spec. To spec.

igm Robotic Systems, Inc.  Menomonee Falls, WI

RDMK-1002 RTe 456, 476, 496 59, 67, 75 HS/TS 6, 7, 8 3 1,320-2,200 To spec. 48 x 118
P2W -10 RTe 456, 476, 496 59, 67, 75 Single axis 6 1 400-2,000 To spec. 36 x 36
P2W-20 RTe 456, 476, 496 59, 67, 75 HS/TS 6 3 2,200 To spec. 28 x 59
RST RTe 456, 478, 496, 477, 497, 459, 479, 499, 478, 498 59, 67, 75, 87, 94, 102 RP HS, RWM2 Skyhook 6, 7, 8 1- 5 22,000 To spec. To spec.
RSH, RTSV, DM RTe 456, 478, 496, 477, 497, 459, 479, 499, 478, 498 59, 67, 75, 87, 94, 102 HS, L-Arm 6, 7, 8 3-7 44,000 To spec. To spec.
RSX 502/1002 RTe 476, 496 67, 75 2 axis Skyhook 2 Stations 6, 7, 8 5 1,100-2,200 To spec. To spec.
TLA3 RTe 456, 478, 496, 477, 497, 459, 479, 499, 478, 498 59, 67, 75, 87, 94, 102 HS, L-Arm 6, 7, 8 3-7 50 tons To spec. To spec.
P2W-30 RTe 456, 476, 496 59, 67, 75 2 axis Tilt/Rotate 6 5 330-2,200 To spec. To spec.