Tube & Pipe Buyers' Guide



 Description Dimensions Material Shapes Production Process
OD Min OD Max Wall Thickness Min Wall Thickness Max Schedule Length Max Ferrous Nonferrous Round Square Rectangular Oval/Oblong Hexagonal Seamless Welded (From Coil) Welded (From Plate)
Carbon Steel High Strength, Low Alloy High-
Alloy
Steels
Superalloy Aluminum Copper Cupronickel Nickel Titanium Refractory Metals Cold Drawn Hot Finished As Welded Cold Drawn Helical/Spiral Roll Bending UOE
Corrosion Resistant Heat Resistant Wear Resistant

Central Steel and Wire Co.  Chicago, IL

             

Copper & Brass International Corp.  Houston, TX

Heat Exchangers .25 .75
Heat Exchangers .5 6 65

EPIX Tube Co., Inc.  Trotwood, OH

Mechanical Tube .625 3.188 .025 .160 50

Freeport-McMoRan Copper & Gold  Elizabeth, NJ

Mechanical Tube 1.0 4.0 .10 4.0 40 & 80 12+

H & H Tube & Manufacturing Co.  Vanderbilt, MI

UNS C23000, Brass, Red .125 3.25 .010 .260

KJ Tubing Inc  Mentor, OH

 Hx and Process Tube & Pipe  .375  24  .02  1  All  

Metal-Matic Inc.  Minneapolis, MN

Mechanical Tube .375 4.50 .028 .250 52

Michigan Seamless Tube LLC  South Lyon, MI

.75 5.00 .083 .875 52
Mechanical Tube .75 5.00 .083 .875 52
Pressure Tube .75 5.00 .083 .875 52
Pressure Pipe .75 5.00 .083 .875 52

Pittsburgh Tube & Steel  Middlesex Twp., PA

.250 10.00 .028 1.375 40

Shaanxi Rongyuan Industrial Development Co., Ltd.  Xi'an, China

0.079 8.62 0.012 0.473 59.2

Superior Tube Co.  Collegeville, PA

316V (Medical) .010 1.250 .003 .125 20
Nuclear .010 1.250 .003 .125 40
Aerospace .010 1.250 .003 .125 20

T & B Tube Co. Inc.  South Holland, IL

Mechanical Tube .375 3.00 .023 .125 26

Titan Engineering Pte. Ltd.  Singapore, Singapore

Heat Exchangers .25 4 ,05 1 40

United Industries Inc.  Beloit, WI

1 8 .20 120 60

Voest-Alpine Tubular Corp.  Houston, TX

OCTG/Casing 4.5 7 0.142 0.689 42
OCTG/Tube 2.375 4.5 0.114 0.472 42
OCTG/Line Pipe 1.660 6.625 0.125 0.630 45

Voestalpine Tubulars GmbH & Co. KG  Kindberg, Austria

OCTG/Tube 1.660 7.000 .125 .750 42
OCTG/Line Pipe 2.375 6.625 .125 .500 45
Mechanical Tube 1.059 7.000 .102 .787 57.4

Wheatland Tube Co.  Chicago, IL

Mechanical Tube .706 5 .035 .220 40
Mechanical Tube .625 4 .035 .220 40
Mechanical Tube .75 x 1.5 2 x 6 .035 .220 40
Standard Pipe .125 6.625 .068 .280 40 40
Standard Pipe .125 4.5 .095 .337 80 40