Tube & Pipe Mill Machine Buyers' Guide



 
Process
Tube Dimensions
Material
Model or Series Electron Beam ERW High frequency Contact ERW High frequency Induction ERW Rotary Wheel Direct Current DC ERW Rotary Wheel Square Wave Laser Plasma Spiral Welding TIG GTAW OD Minimum Inches OD Maximum Inches Wall Thickness Minimum Inches Wall Thickness Maximum Inches Mild Steel Stainless Steel Aluminum Copper Other Metals Round Square Rectangle Other Shapes

Abbey/OTO products - Fives Bronx Inc.  North Canton, OH

1K-1.5 .375 1.5 .018 .083
2X-2.25 .500 2.25 .020 .095
2K-3.5 .625 3.5 .028 .125
3X-3.5 .750 3.5 .032 .160
3K-3.5 .840 3.5 .042 .203
4X-5.0 1.25 5.0 .42 .188
4K4.5 1.0 4.5 .049 .25
5K-5.625 1.25 5.625 .049 .25
6X6.625 1.9 6.625 .049 .237
6K-6.625 1.9 6.625 .083 .338
7X-7.5 2.375 7.5 .065 .280
7K-7.5 2.375 7.5 .083 .340
8K-8.75 2.875 8.75 .083 .375
12X-12.75 3.5 12.75 .083 .330
12K-12.75 3.5 12.75 .12 .625
16K-16.0 4.5 16.0 .12 .625
20K-20.0 6.625 20.0 .120 .5
24K-24.0 8.625 24.0 .188 .750
27K-27.0 10.75 27.0 .2 .750
36K-30.0 14.0 36.0 .2 1.0

Dreistern Inc.  Telford, PA

RSD 50 .25 2.00 .006 .016
RS 060 .118 1.00 .006 .040
RS 080 .118 1.50 .012 .040
RS 100 .40 2.00 .016 .078
RS 125 .55 3.00 .020 .102
RS 160 .71 4.00 .024 .142
RS 200 1.18 6.60 .028 .200

FD Machinery  Cleveland, OH

 FDL 033  .375 1.25 .024 .118
 FDL 042 .375 1.654 .024 .157
 FDL 050  .375 2.00 .024 .177
 FDL 076 .750 3.00 .031 .236
 FDL 089  1.00 3.500 .031 .276
 FDL 114  1.250 4.500 .039 .315
 FDM 127  1.500 5.000 .039 .315
 FDM 140  1.500 5.500 .059 .315
 FDM 168  1.890 6.625 .059 .394
 FDM 170  3.500 8.625 .079 .472
 FDH 200  4.000 10.000 .079 .472
 FDH 210  4.500 10.750 .079 .512
 FDH 250  5.500 12.750 .098 .551
 FDH 280 5.500 14.000 .098 .551
 FDH 320  6.625 16.000 .098 .630
 FDH 360 6.625 18.000 .098 .630
 FDH 400  8.625 20.000 .118 .630
 FDH 480  8.625 24.000 .118 .750

Henry Engineering Ltd.  Auckland, New Zealand

 Pipe Mill  16  60 .125  2

Kent Corp.  North Royalton, OH

MTM 040 C .240 1.110 .010 .047
MTM 040 C Broom Handles .400 1.110 .008 .024
MTM 040 C Window .22 x .260 1.20 x .260 .008 .020
MTM 040 C Wire .100 .150 .020 .033
MTM 040 Radiator - Intercoolers .7 x .60 1.50 x .1 .008 .047
MTM 050 C .400 1.500 .020 .098
MTM 060 C .500 2.500 .024 .120
MTM 070 C .630 3.000 .035 .157
MTM 080 C .830 3.150 .040 .197
MTM 090 C 1.000 3.500 .040 .217
MTM 100 C 1.300 4.500 .050 .217
MTM 120 C 1.660 5.000 .060 .236
MTM 130 C 2.500 6.620 .060 .276
MTM 160 C 3.500 8.630 .079 .315
MTM 170 C ST HF 4.500 10.000 .100 .315

Liburdi Automation Inc.  Dundas, ON Canada

Linear Cage Forming SCF 30-80 1.181 3.150 .039 .236

Mill Masters Inc.  Jackson, TN

Spectrum Series S-626 .24 1.02 .010 .040
Spectrum Series S-1976 .75 3.00 .015 .118
Premier Series P-626-T .24 1.02 .010 .040
 Elite, Ultra; Premier; Quantum  .20  6.0 .005  .118

Nakata Manufacturing Co. Ltd.  Osaka, Japan

FFX 2 26 .031 1.000

Officine MTM S.p.A.  Spinea (Venezia), Italy

 MTM 040 C .240  1.100  .012  .047
 MTM 050 C  .400  1.500  .020  .098
MTM 060 C  .500  2.500  .024  .120
 MTM 070 C  .630  3.000  .035  .157
 MTM 080 C  .830  3.150  .040  .197
 MTM 090 C  1.000  3.500  .040  .217
 MTM 100 C  1.300  4.500  .050  .217
 MTM 120 C  1.660  5.000  .060  .236
 MTM 130 C  2.500  6.620  .060  .276
 MTM 160 C  3.500  8.630  .079  .315
 MTM 170 C  4.500  10.000  .100  .315
 MTM 040 C RAD W - Radiator - Intercoolers  .492 x .060  1.400 x .080  .008  .016

Rafter Equipment Corp.  Strongsville, OH

RT-1000 .250 1.000 .010 .049
RT-1250 .250 1.250 .020 .065
RT-1500 .375 1.750 .020 .083
RT-2000 .500 2.500 .020 .120
RT-2000S .500 3.000 .028 .135
RT-2500 .075 3.000 .032 .165
RT-3000 .750 4.000 .032 .188
RT-3500 1.000 5.000 .048 .250
RT-4500 1.250 6.000 .060 .300
RT-6000 2.500 8.625 .065 .440
RT-8000 4.000 12.750 .065 .500
RT-9000 6.625 16.000 .120 .625

SEUTHE GmbH  Hemer, Germany

Conventional RS 16 .185 .630 .019 .060
Conventional RS 30 .375 1.181 .024 .160
Conventional RS 60 .630 2.500 .035 .250
Conventional RS 127 1.496 5.000 .059 .320
Conventional RS 168 1.900 6.625 .079 .400
Conventional RS 273 3.000 10.750 .118 .500
Conventional RS 406 5.500 16.000 .157 .625
Conventional RSE 25 .250 1.000 .020 .100
Conventional RSE 60 .625 2.500 .028 .118
Conventional RSE 127 1.500 5.000 .040 .250
Cage Forming 90 Round 1.625 3.500 .177
Cage Forming 127 Round 1.900 5.000 .250
Cage Forming 168 Round 2.375 6.625 .315
Cage Forming 220 Round 3.000 8.625 .375
Cage Forming 406 Round 5.500 16.000 .625
Cage Forming 240 Square .750 x .750 2.375 x 2.375 .125
Cage Forming 400 Square 1.500 x 1.500 4.000 x 4.000 .250
Cage Forming 600 Square 2.375 x 2.375 6.000 x 6.000 .312
Cage Forming 1000 Square 4.000 x 4.000 9.875 x 9.875 .500
Cage Forming 1600 Square 5.875 x 5.875 15.750 x 15.750 .625

T&H Lemont  Countryside, IL

WU-8 .090 .375 .006 .035
WU-11 .150 .750 .010 .050
WU-11M .250 1.000 .020 .065
WU-15 .375 1.750 .020 .083
WU-20 .500 2.500 .020 .134
WU-25 .750 3.500 .025 .160
WU-35 1.000 4.500 .060 .240
WU-40 1.500 5.500 .060 .280
WU-50 2.000 6.625 .080 .330
WU-60 2.000 8.625 .110 .375

TTM Laser S.p.A.  Cazzago San Martino, Italy

 FL 170 3D FIBER  .5  6.6   .3
FL 300 3D  .75  12    .3
 FL 400 3D  1  16    .4
 FL 600 3D  3.4  24    .4
 FL 800 3D  5.9  32    .4

Thermatool Corp.  East Haven, CT

View Details .125 24.0 .010 1.0

Universal Tube & Rollform Equipment Corp.  Perrysburg, OH

190-6 2.362 7.480 .240
 76 1  3  .032  .166

Yoder - A Member of the Formtek Group  Cleveland, OH

12" Pipe Mill 4.500 12.750 .083 .625
16" Pipe Mill 4.500 16 .120 .625
26" Pipe Mill 6.625 28 .120 1.000
6" Pipe Mill 2.375 6.625 .065 .438
8" Pipe Mill 2.875 8.625 .083 .500
M-1-1/2 & QVW-150 .313 1.250 .018 .049
M-2 & QVW-200 .500 2.250 .018 .095
M-2-1/2 & QVW-250 .500 3 .018 .134
W-10S/W-15S .188 .500 .020 .040
WH-150 .375 1.500 .020 .083
WH-200 .500 3.000 .020 .135
WH-250 .750 3.500 .035 .180
WH-350 1.250 5.500 .065 .375

olimpia 80  Borgonovo V.T. (PC), Italy

Compact .197 .787 .016 .079
Compact S .197 .984 .016 .079
30/35R .315 1.669 .020 .089
30/35 .472 1.669 .028 .098
50/60 .630 2.00 .028 .118
60/90 .984 3.500 .031 .197
100/170 2.374 6.626 .047 .315
150/300 4.000 12.752 .079 .500
180/450 5.91 16.00 0.118 .630
250/600 8.626 24.000 .157 .709
250/600 8.626 24.00 .157 .709
Linear Cage Forming SCF 20-60 1.181 3.150 .039 .236
Linear Cage Forming SCF 30-80 1.181 3.15 .039 .236
Linear Cage Forming SCF 80-200 3.150 7.874 .079 .500
Linear Cage Forming SCF 100-250 3.94 9.84 .118 .500
Linear Cage Forming SCF 100-250 4.724 11.811 .157 .630
Linear Cage Forming RCF 40-101 1.575 4.00 .039 .197
Linear Cage Forming RCF 76-168 3.00 6.626 .059 .315
Linear Cage Forming RCF 120-310 5.00 12.205 .098 .500
Linear Cage Forming RCF 170-410 6.69 16.00 .118 .630
Linear Cage Forming RCF 270-610 10.630 24.00 .118 .787