- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Welding wires designed for single- or multilayer surfacing
- January 13, 2014
- Product Release
- Consumables
Sandvik offers three welding wire grades for GTAW, plasma arc welding, GMAW, and SAW.
Characterized by its very low cobalt, vanadium, and boron content and enhanced ferrite content, Sandvik 24.13.LHF has high resistance to hot cracking. The wire is recommended for first-layer weld cladding procedures and dissimilar joining of stainless to low-alloyed or nonalloyed steels, wrought iron, and cast iron. It is also suitable for overlay welding of carbon and low-alloyed steels, where a 304/304L deposit is required.
Sandvik 24.13.LNb offers stability at high temperatures. An overalloyed filler metal, it is recommended for overlay welding of carbon and low-alloy steels that require a type 347 overlay. Its weld deposit is niobium stabilized and thus resistant to carbide precipitation and resultant intergranular corrosion.
Sandvik 24.16.3.L is suitable for welding on oil and gas pipelines and valves. The corrosion resistance of the weld overlays is at the same level as the 316L base metal. The wire is suitable for the buffer layer on steel in multilayer techniques.
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI