July 10, 2013
GTAW rod eliminates gas purging in pipe welding
Cor-Met Inc. offers QWP flux-coated GTAW rod for pipe welding. It forms a slag on the backside of a pipe, protecting the weld from oxidation and eliminating the need for gas purging and backing. Available grades are 308H, 308L, 309L, 316L,... Read more...

Article

August 8, 2007
Flood-weld forging dies and large castings
COR-MET has been manufacturing flux cored wire and electrodes since 1972, specializing in high deposition alloys for the repair of Forging Dies and Large Foundry Castings. The Flood Welding Procedure will deposit up to 60 lbs per hour of weld... Read more...