July 10, 2013
GTAW rod eliminates gas purging in pipe welding
Cor-Met Inc. offers QWP flux-coated GTAW rod for pipe welding. It forms a slag on the backside of a pipe, protecting the weld from oxidation and eliminating the need for gas purging and backing. Available grades are 308H, 308L, 309L, 316L,... Read more...