News

February 27, 2014
Davi variable-axis plate roll purchased by Edmonton Exchanger
Davi has announced the purchase of an MAV 3060 variable-axis plate roll by Edmonton Exchanger, Edmonton, Alb. The machine has a capacity of 10 ft. by 3.25 in. Read more...

Product

July 31, 2013
Three-roll plate machine fabricates storage tanks, pressure vessels
Davi has designed a MAV three-roll plate roll machine with variable axes for a fabricator of storage tanks and pressure vessels in Turkey. The machine has a capacity of 10 ft. by 5.375 in. Read more...

Article

June 3, 2013
Plate-rolling out the weakest links
When certain customers order a rolled and welded cylinder from North Shore Steel’s plate processing division, they can have their product delivered within not weeks, but about four days. This isn’t common in a sector where... Read more...

Product

March 6, 2013
Four-roll machine's overhead support lifts 100 tons
Davi has supplied a four-roll machine that it says is the largest in the world with the heaviest overhead support ever made. The overhead support is able to lift 100 tons — the equivalent of an Airbus 330. Read more...

News

January 24, 2013
Davi earns highest quality degree from ThyssenKrupp
Following annual supplier evaluations, ThyssenKrupp has assigned an A rating, the highest supplier degree, to Davi, Dallas. ThyssenKrupp purchased four Davi plate rolls in 10 years for its facility in South America. The company uses the... Read more...

News

October 23, 2012
Davi delivers large-capacity plate roll to wind tower manufacturer
Davi has installed a four-roll plate roller with a capacity of 4,000 by 145 mm at Bladt, Denmark's largest wind energy fabricating company. The machine cold-rolls monopiles for offshore wind towers. The machine is automated via iRoll,... Read more...

News

July 24, 2012
Davi completes production of heaviest plate roll
Dallas-based Davi has manufactured and commissioned what it says is the heaviest four-roll machine ever built. The 13.12-ft. by 10-in. machine was dismantled and delivered to the customer via 17 trucks. It will be used for the production of... Read more...

Article

June 2, 2011
Plate rolls keep rolling heavier plate
Plate rolls have gotten seriously big. Machine pits are deeper, the frames massive, the rolls ever larger. Certain machines have specifications stating they can roll plate of certain yield strengths to 4, 6, and 7, even 11 inches—cold.... Read more...

Article

January 13, 2009
EuroBLECH 2008: A celebration of metal fabricating and forming
What does a European metal fabricating and forming tradeshow mean for a U.S. fabricator? Apparently, a whole lot. "It means everything. It has influenced who we are," said Don Begneaud, speaking about his company, BEGNEAUD Manufacturing, in... Read more...

Article

January 15, 2008
Heavy bending
A 4- by 4-foot, 1/4-inch-thick plate can weigh more than 113 pounds. Even a 4- by 4-ft., 3/16-in.-thick plate can weigh more than 85 lbs. Such weights can create challenges on the press brake. When bending material thicker than 10-gauge, at... Read more...

Article

October 9, 2007
Dealing with Mother Nature's wrath
Protecting a two-mile-long, 10-lane bridge from earthquake damage is not an easy task. Replacing the eastern span of the San Francisco-Oakland Bay Bridge requires the talent and time of numerous design firms and fabricators and tens of thousands... Read more...