Presquared tool steel saves time for tool- and diemakers
Accu-Squareâ„¢ presquared tool steel from Diehl Steel helps save time for tool-, die-, and moldmakers by reducing or eliminating the need for further squaring of the blocks. The tool steel comes presquared on all six sides to a tolerance... Read more...