Article

March 25, 2015
WorldAutoSteel Guidelines for AHSS shed light on lightweighting
The international steel industry has seized the opportunity to create new families of alloys with higher strength and greater formability than those that existed just a few years ago to meet higher requirements for vehicular fuel efficiency.... Read more...

News

January 12, 2010
Web site shares sheet metal product, materials guidance
Engineering Quality Solutions Inc., a technical consulting firm in Southfield, Mich., is providing information to assist Web site visitors with sheet metal product application and materials utilization. Visitors to www.eqsgroup.com have access... Read more...

Article

July 15, 2008
Forming AHSS: Playing by new rules
Mention a certain material is predicted to overtake mild steel as the auto sector's most popular material in 10 years, and people take notice. That's been Peter Ulintz's experience in recent years. As advanced product engineering manager for... Read more...

Article

September 13, 2005
Introduction to advanced high-strength steels
Part I of this two-part series presented an overview of advanced high-strength steels (AHSS). This article addresses issues encountered when processing these grades. Using AHSS in appropriate applications offers opportunities for reduced... Read more...

Article

September 13, 2005
Introduction to advanced high-strength steels - Part II
Part I of this two-part series presented an overview of advanced high-strength steels (AHSS). This article addresses issues encountered when processing these grades. Using AHSS in appropriate applications offers opportunities for reduced... Read more...

News

September 13, 2005
EQS president elected NADDRG secretary
Engineering Quality Solutions Inc. President Daniel Schaeffler has been elected secretary of the North American Deep Drawing Research Group (NADDRG). NADDRG fosters and encourages sheet metal forming research in materials, tool and die design,... Read more...

Article

August 9, 2005
Introduction to advanced high-strength steels - Part I
Editor's Note: A version of this article appeared in the November 2004 issue of STAMPING JournalĀ® . Several new commercialized and near-commercialized advanced high-strength steels (AHSS) that exhibit high strength and enhanced formability... Read more...