Product

June 14, 2005
Flap brushes remove surface contaminants, oxidization
Even Cut Abrasive Co. offers flap brushes made from flexible, open-structured nylon web with embedded resin and aluminum oxide grain. The brushes are suitable for removing surface contaminants and oxidization and for blending and producing fine... Read more...

Product

April 12, 2005
Flap wheels designed for consistent cutting, finishing
Even Cut Abrasive Co. offers balanced flap wheels designed to produce consistent cuts and finishes. Radially mounted around a metal shank or hub, the wheels are suitable for contouring, blending, finishing, deburring, and polishing both ferrous... Read more...