December 7, 2004
Penna Flame Industries increases capabilities
Penna Flame Industries has added induction hardening to its surface hardening capabilities. The company also now offers single-tooth contour gear hardening, a process intended to improve gear teeth strength and wear with minimal distortion. Read more...