January 13, 2014
Welding wires designed for single- or multilayer surfacing
Sandvik offers three welding wire grades for GTAW, plasma arc welding, GMAW, and SAW. Characterized by its very low cobalt, vanadium, and boron content and enhanced ferrite content, Sandvik 24.13.LHF has high resistance to hot cracking. The... Read more...

Product

December 14, 2011
Coated stainless steel strip designed for electronic component manufacturers
Sandvik has introduced Sandvik Santronicâ„¢, a coated stainless steel strip designed for electronic component manufacturers. It can serve as an alternative material for postprocessed electroplated parts in stainless steel or copper-based alloys.... Read more...

Product

December 11, 2007
Overlay welding strip intended to reduce production time
Sandvik says its new welding strip, Sandvik 24.29.5.LCu, reduces production time by half in overlay welding applications. The material allows users to attain the required grade for 904L overlay in a single weld using a standard flux, the company... Read more...