Select-Arc Inc. Showroom

Visit Select-Arc Inc.  

 

   Found 25 results for "Select-Arc Inc."...

      Just show me: Everything | Articles | News | Products

Product

March 9, 2015
Electrode welds thin exhaust components
Select-Arc Inc. has introduced a metal-cored ferritic stainless steel electrode designed for use on thin materials in automotive applications. It can weld aluminized or other coated components on 0.03-in. material with no burn-through. The... Read more...

Product

February 9, 2015
Electrode welds zinc-galvanized, primer-coated steels
Select-Arc Inc. has introduced a premium carbon steel, composite metal-cored electrode designed to weld zinc-galvanized and primer-coated steels. Superior arc stability produces spatter-free welds at high travel speeds, the company states.... Read more...

Product

January 15, 2015
Electrode welds aluminized material
Select-Arc Inc. has introduced Select FP 409Ti, a composite metal-cored electrode designed for welding ferritic stainless steel, particularly on thin-section, aluminized material. Titanium acts as the stabilizing agent to provide oxidation and... Read more...

Product

December 22, 2014
Updated catalog includes 14 new welding electrodes
Select-Arc Inc. has added 14 new welding electrodes to its updated full-line catalog of premium flux-cored and metal-cored welding electrode products. The 108-page catalog provides detailed information on more than 180 Select-Arc carbon... Read more...

Product

October 15, 2014
Electrode welds plates with surface contaminants
Select-Arc Inc. has introduced Select 70CRP, a flux-cored carbon steel electrode designed for the welding of structural plate with surface contaminants, such as rust and weldable primers. It welds on these surfaces with minimal porosity and... Read more...

Product

September 19, 2014
Metal-cored electrode engineered for low-temperature stress relief
Select-SAI Inc. has introduced Select 70C-6 SR, an E70C-6MJ-H4 gas-shielded, metal-cored electrode designed for low-temperature service requirements. The wire provides excellent weldability with a low slag, resulting in a smooth arc transfer... Read more...

Product

June 18, 2014
Flux-cored, gas-shielded electrode introduced
Select-Arc Inc. has introduced an E71T-1 flux-cored, gas-shielded electrode designed for weldability over a variety of parameters. Select 707 is an all-position wire for welding at low- or high-current settings that exhibits a smooth arc... Read more...

Product

September 19, 2013
Flux-cored electrode designed for stress-relieved applications
Select-Arc Inc. offers a gas-shielded, flux-cored electrode designed for welding carbon and certain low-alloy steels in applications in which excellent mechanical properties are required in both the as-welded and stress-relieved conditions.... Read more...

Product

July 22, 2013
Nickel-alloy electrode engineered for rigorous environments
Select-Arc Inc. has introduced a gas-shielded, flux-cored, nickel-based electrode designed to tackle critical welding applications in demanding environments such as desalination plants, petrochemical facilities, power generation plants, and... Read more...

Product

February 16, 2012
Weathering steel electrodes designed for bridge, building construction
Select-Arc Inc. offers two low-alloy steel electrodes designed for applications requiring the coloration and corrosion resistance of the weathering type of structural steels. Select 810-W is a gas-shielded, flux-cored, all-position wire... Read more...

Product

November 10, 2011
Martensitic electrodes introduced
Select-Arc Inc. has introduced two gas-shielded, flux-cored stainless steel electrodes in 0.045- and 0.0625-in. diameters. Select 410-AP is an all-position wire that delivers flat, well-washed beads with minimal weaving. It produces very... Read more...

Product

January 17, 2011
Stainless steel electrodes designed for use in specific industrial applications
Select-Arc Inc. has introduced two gas-shielded, flux-cored, austenitic stainless steel electrodes designed for use in specific industrial welding applications. SelectAlloy 309H-AP is composed of nominal weld metal of 24 percent chromium... Read more...

Product

November 15, 2010
Stainless steel electrodes designed for industrial welding applications
Select-Arc Inc. has introduced two gas-shielded, flux-cored, austenitic stainless steel electrodes designed for use in industrial welding applications. SelectAlloy 307-AP is composed of nominal weld metal of 19 percent chromium, 10 percent... Read more...

Product

March 5, 2010
Nickel electrode resists crevice corrosion, pitting
Select-Arc Inc. has introduced a gas-shielded, flux-cored, nickel-based electrode designed to resist crevice corrosion and pitting. SelectAlloy C276-AP has been developed to weld nickel-chromium-molybdenum to itself or to other nickel-based... Read more...

Product

November 11, 2008
Stainless steel electrodes suitable for surfacing, welding over gaps
Select-Arc Inc. has introduced two self-shielded, flux-cored stainless steel electrodes designed to weld stainless steels and for the cladding of carbon steels. The lower penetration of the wires makes them suitable for surfacing and for welding... Read more...

Product

August 12, 2008
Electrodes designed for tubular welding
Select-Arc Inc. manufactures tubular welding electrodes. The company's line of welding wires comprises flux-cored and metal-cored products, including carbon steel, low-alloy, stainless steel, nickel-alloy, and hardsurfacing electrodes.... Read more...

Product

June 17, 2008
Metal-cored electrode designed for stainless, other austenitic steels
Select-Arc Inc. has introduced a composite metal-cored electrode for GMAW of stainless and certain other types of austenitic steels. The composite nature of SelectAlloy 307EU-C provides high deposition rates, fast travel speeds, and a weld... Read more...

Product

March 11, 2008
Hardsurfacing electrodes have extended wear life
Select-Arc Inc. has introduced two complex carbide hardsurfacing electrodes designed to extend wear life by 33 percent over standard chromium carbide alloys, reports the company. SelectWear 63 is an open-arc wire produced to yield a deposit of... Read more...

Product

January 15, 2008
Stainless steel electrodes designed for elevated travel speed butt, lap, fillet welds
Select-Arc Inc. has introduced two gas-shielded metal-cored, stainless steel electrodes designed for making butt, lap, and fillet welds at elevated travel speeds. The electrodes offer a maximum carbon content of 0.03 percent, to minimize carbide... Read more...

Product

January 9, 2007
Metal-cored electrode designed for cast irons
Select-Arc's 2216-C metal-cored electrode is designed to weld cast irons that demand increased strength at relatively higher temperatures. It is suitable for joining cast irons to alloy and carbon steels. The electrode features a 41 percent... Read more...

Product

August 8, 2006
Electrode welds steel requiring 70,000-PSI minimum tensile strength
The Select 711 gas-shielded, flux-cored carbon steel electrode from Select-Arc Inc. welds steels that require a minimum of 70,000-PSI tensile strength. The all-position electrode produces good arc drive and bead shape, the company states. The... Read more...

Product

July 11, 2006
Flux-cored stainless steel electrodes designed for demanding environments
Select-Arc Inc. offers three gas-shielded, flux-cored stainless steel electrodes designed for welding in demanding environments. The SelectAlloy 308H-AP, 309LMo-AP, and 347-AP electrodes feature flat, well-washed beads that can be achieved with... Read more...

Product

April 11, 2006
Metal-cored electrodes suitable for weldments requiring painting
Select-Arc Inc. offers two carbon steel, gas-shielded, composite metal-cored electrodes that have a high tolerance of mill scale and rust. Both are suitable for weldments that require painting. The Select 70C-6LS electrode minimizes silicon... Read more...

Product

February 7, 2006
Electrodes meet military specifications
Select-Arc Inc. offers two low-alloy steel, gas-shielded, flux-cored electrodes with military specification approvals. The Select 820-Ni1 produces 1 percent nickel weld deposit and welds steels that require low-temperature CVN toughness and... Read more...

Product

December 13, 2005
Metal-cored electrodes designed for stainless steel
Select-Arc Inc. has added three ferritic metal-cored, composite electrodes, the Select 409C, Select 409C-Cb, and Select 409C-Ti, to its stainless steel product line. The 409C is suitable for welding ferritic stainless steel sheet and thin-gauge... Read more...