October 1, 2014
Electric tube hone handles bore IDs up to 35.41 in.
Sunnen’s new HTR all-electric job shop tube hone combines servo precision and cycle automation features with constant spindle power and 0.004-in. stroke repeatability to hone blind bores or correct tight spots in a bore without operator... Read more...

Product

May 7, 2014
Honing process produces less than 2-micron cylindricity in long, small-diameter bores