- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
A trophy fit for Titletown
Packer fandom reigns at Wisconsin metal fabricator
- By Amanda Carlson
- January 27, 2017
- Article
- Arc Welding
Green Bay Packer fans and tailgating go together like cheese curds and beer. Whether you love them, hate them, or envy them, you have to admit that these fans exist in a class by themselves. What other fan base willingly subjects their bodies to the subzero outdoor temperatures, sometimes paired with snow, freezing rain, or whipping winds—conditions typically fit only for Arctic creatures—all in the name of tailgating and watching football?
Hailed by Forbes as the best fans in the NFL, loyalists of the team wear their fandom as a badge of honor. While their bravado doesn’t always sit well with opposing fans, like it or not, being a Packer fan, especially on game day in Green Bay, is pretty freaking cool.
Game day tailgating is more than a pregame meal with beverages; it is an opportunity for the fans to come together, clink glasses (or cans, steins, or flasks) and celebrate their common allegiance to the green and gold. Case in point, Lambeau Field, this fan base’s version of the Sistine Chapel, sits cozily in a residential neighborhood where many of the houses have been purchased by devoted fans and converted into tailgate party crash pads for supporters who want to live it up on game day, avoid expensive hotels, or just bask in the glow of their favorite landmark.
De Pere, Wis.-based Robinson Metal is located in the heart of Packers country and employs a good number of Packers fans (as well as an occasional Bears fan). Eight years ago it purchased a home just outside of Lambeau Field; converted it into a tailgate-friendly space; and currently uses it to entertain customers and vendors and give employees a place to hang out with co-workers and their families before game time.
“We open our tailgate house four hours before kickoff. Down one full wall of the garage there’s a huge hot buffet of food and beverages. We fill the whole yard with picnic tables and everyone just dresses for whatever kind of weather it is. The whole party pretty much takes place outside. The house was converted and remodeled basically to be used for bathrooms and to allow people to change into their warm, heavy game gear. There’s still a small living room and kitchen where people can congregate and get warm during the colder days,” explained Steve Hartliep, sales and marketing manager at Robinson Metal.
It’s Not a Tailgate Without a Trophy
Being that it is located in “Titletown,” the tailgate location wouldn’t be complete without a giant replica of the Vince Lombardi Trophy.
The company had been commissioned by a couple of local groups to fabricate some monuments to commemorate Packers history for placement around town. It also fabricated a replica Lombardi Trophy for a local bar.
“We decided, why not make something for ourselves for our tailgate house? That’s how it spawned,” Hartliep said.
The base of the 10-foot structure is made of 3⁄16-inch stainless steel and mounted on a slab of concrete. The ball is made out of 12-ga. 304-2B stainless and has a DA finish on the exterior. The internal skeleton structure of the football is made out of bar stock.
“Fabricating the football was a real challenge because there’s curving, a circumference, and diameter that you have to hold to. Then you have a point-to-point longitudinal structure that you have to keep in place,” Hartliep said.
The football was made out of four sections that were spun and formed. Those four sections were blocked together on the skeletal structure, bolted to it, and then tack welded from the inside.
The finished product weighs roughly 600 lbs. and required approximately 40 hours of production labor. For the green and gold-loyal shop, it was certainly a labor of love that makes tailgating a lot of fun.
“The trophy is a major focal point for every one of our game day tailgate parties. Group after group goes up to the trophy to get their pictures taken. It has made an appearance in numerous Christmas cards for people that we know and families that have used it. In fact, my family goes every year and gets a new picture taken with the trophy, so it’s definitely a focal point.”
The only thing better than Robinson’s replica trophy would be for the Packers to bring home the real thing.
Robinson Metal Inc., 920-494-7411, www.robinsonmetal.com
About the Author
Amanda Carlson
2135 Point Blvd
Elgin, IL 60123
815-227-8260
Amanda Carlson was named as the editor for The WELDER in January 2017. She is responsible for coordinating and writing or editing all of the magazine’s editorial content. Before joining The WELDER, Amanda was a news editor for two years, coordinating and editing all product and industry news items for several publications and thefabricator.com.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Educating, rather than just training, tomorrow's workforce
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,