- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Rocklinizer Automation system from Rocklin Mfg. brings turnkey automation to hard surface coating
- January 31, 2022
- Product Release
- Metals/Materials
Rocklin Manufacturing has introduced Rocklinizer Automation, the first turnkey automation system in its line of carbide application equipment. The company’s proprietary Rocklinizer spark deposition process applies extremely hard and wear-resistant coatings onto steel surfaces, typically through a hand-held, manual coating process.
The system achieves precisely controlled deposits, from 0.0001 to 0.010 in., in three steps:
- Measure and position the part to be coated in the large X-Y frame.
- Insert the electrode into the applicator and adjust the power and speed to desired levels.
- Input the part dimensions on the integrated touchscreen PC and trigger the coating process.
Unlike welding or metal spraying, the process generates minimal heat, and the electrode material will not separate or flake off, according to the company. After application, no heat treatment, grinding, or other surface treatment is necessary.
The carbide application process helps boost grip on tube bending dies, collets, and robot grippers; minimize die casting wear; eliminate slug pullback in punching and stamping; restore tolerances in bearings and shafts; and increase the life of cutting tools.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI