- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Grieve 2,000-degrees-F, inert-atmosphere, heavy-duty box furnace heat-treats titanium
- March 4, 2020
- Product Release
- Shop Management
No. 954 is an electrically heated, 2,000-degrees-F, inert-atmosphere, heavy-duty box furnace from Grieve, currently used for heat-treating titanium at a customer’s facility. To heat the load, 57 kW are installed in nickel-chrome wire coils supported by vacuum-formed ceramic fiber.
Workspace dimensions are 30 in. wide by 48 in. deep by 30 in. high. The oven’s 7-in.-thick insulated walls comprise 5 in. of 2,300-degrees-F ceramic fiber and 2 in. of 1,700-degrees-F ceramic fiber, while the 6-1/2-in. floor insulation comprises 4-1/2 in. of 2,300-degrees-F firebrick and 2 in. of 1,200-degrees-F block insulation.
The unit is equipped with a roof-mounted, heat-resisting-alloy recirculating fan and powered by a 1-HP motor with V-belt drive. It features a motor-operated vertical lift door, 100-lb.-capacity alloy-loading cart with cast-alloy roller rails, 3-1/2-in.-dia. cast-alloy rollers, and a roller rail loading table with 4-in.-dia. cast-iron rollers.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, owner of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,