- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Welding procedure specifications for beginners
- By Paul Cameron
- Updated February 29, 2024
- October 23, 2014
- Article
- Arc Welding
Q: Recently I was given a weld procedure specification (WPS) from a contractor to review. It’s still lying on my desk. Do you have any tips for a beginner like myself on how to review a WPS?
A: It’s time to pick up that WPS off your desk and give it a good, hard look. The first thing you need to arm yourself with is the correct code or standard. The WPS is going to state which code or standard it complies with. You most likely need to get familiar with ASME Section IX or AWS D1.1 Sections 3 and 4, or both.
Does it reference a procedure qualification report (PQR), or is it considered prequalified? It is important to make sure that the WPS states how it was qualified.
Review the Joint
Take a look at the joint design. Does the joint on the WPS match the joint referenced? Is backing required? Is the joint within the stated tolerances?
Ensure the base metal of the joint matches the base metals listed on the WPS, which may require a little homework. Your code should list materials by group or P-numbers. Also review the filler metal/flux/shielding listed and witness which is used.
Heat Treating and Parameters
Are there preheat or postweld heat-treat requirements? How will you measure them? Are the welding parameters such as current, voltage, travel speed, and number of passes being used within the range of the ones that are listed? How will you measure them?
A WPS is really a recipe for how a particular weld is going to be made. All the ingredients need to match, and when they don’t, even beginners need to stand up and get the attention of someone who will get your welding back on track. Don’t be intimidated by a WPS. Break it down section by section, and simply ensure that what is noted matches what is being done on your project.
About the Author
Paul Cameron
Braun Intertec
4210 Highway 14 East
Rochester, MN 55904
About the Publication
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Building a successful welding program from the ground up
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,