Senior Sales Application Engineer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Consumables Corner: Examining weld cracking, Part II—Stress, hydrogen cracking
- By Jay Ginder and Jerry Mathison
- July 16, 2014
- Article
- Consumables
Editor’s Note: This is the second column in a two-part series.
Q: I work in a midsized job shop, and we weld with the FCAW, GMAW, and SMAW processes. Occasionally we encounter weld cracking issues. What causes weld cracking, and what can I do to prevent it?
A: Stress cracking is similar to hot cracking because it usually produces a longitudinal crack, but it can also be transverse, especially in circumferential welds where the stress is even higher. Stress cracks result when the residual stress of welding exceeds what the weld or base metal can tolerate. In many cases, it also can be attributed to an undersized weld bead.
You can address stress cracking by increasing the weld size, improving joint fit-up to eliminate gaps, and applying or increasing preheat temperature. Preheating slows down the cooling rate, allowing the stresses in the welded area to relieve themselves over a longer period of time. All these suggestions address the reduction of residual stresses during welding.
Hydrogen cracking is sometimes referred to as delayed cracking because it can occur up to 72 hours after the welding is completed. These cracks can occur in the weld metal or heat-affected zone (HAZ), which is the area adjacent to the weld that didn’t melt. Hydrogen cracking runs transverse to the weld 99 percent of the time. It occurs in the presence of four criteria:
- Susceptible microstructure
- Tensile stress
- Hydrogen inducted into the steel
- Steel temperature at 300 degrees and less
To prevent hydrogen cracking, apply preheating or increase the preheating and interpass temperature. This will slow down the cooling rate and allow the excess hydrogen to diffuse before being trapped in the weld metal. The amount of preheat needed will depend on the material type, thickness, and the amount of stress in the weldment. Recommended preheat tables for the various types of steel are available from you filler metal or steel supplier. Depending on its size, you could also hold the weldment above 300 degrees F for a few hours after the welding is completed.
Finally, reduce the amount or source of available hydrogen. This could be as simple as keeping the base material clean and dry and using a filler metal that is low in hydrogen.
About the Authors
Jay Ginder
Filler Metal Manufacturing Center 801 Wilson Ave.
Hanover, PA 17331
Jerry Mathison
Senior Sales Application Engineer
411 S. Ebenezer Road
Florence, SC 29501
843-669-4411
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
Three ESAB welding machines win Red Dot Awards for product design
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,