Independent welding consumables professional
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Consumables Corner: The reasons for and misconceptions about preheating steel
- By Nino Mascalco
- June 10, 2014
- Article
- Consumables
Q: We are expanding our job shop and adding the capability to work with much heavier structures, including considerably thicker materials. Some of these jobs specify high-strength materials and preheating. Some of our welders claim preheating is performed to remove water from the steel. Can you expand on this?
A: This is an excellent topic for discussion! Preheating and postweld stress relief are key points when it comes to welding thicker material sections or high-strength steels (HSS). More often than not, the reasons given for these requirements are misunderstood or simply incorrect.
Let’s start by clarifying one fundamental point: Steel does not contain water. When you heat steel with a torch, water will form several inches away in all directions from the flame. This occurs because the gas being burned to produce the flame is a hydrocarbon, which is composed of hydrogen, oxygen, and carbon. When consumed in a chemical reaction such as a flame, the byproducts are mainly carbon dioxide and water. As the hot gases from the flame containing this water get farther away from the flame, the cooler temperatures of the ambient air and steel surface cause the water to condense out of the gases and collect on the surface of the steel plate. This phenomenon appears to be water coming out of the steel, which we know is impossible. Unfortunately, common phrases such as "sweating the steel" or "drive the moisture out" mislead people in the industry as to what is actually occurring.
Preheating steel before welding is necessary for two reasons: First, it raises the overall temperature of the material, which results in a slower cooling rate of the base materials and the weld. Thicker sections of steel, generally 1/2 inch or more, and HSLA (high-strength low-alloy) steels are susceptible to formation of brittle microstructures if the weld cools too quickly. This brittle microstructure we are trying to avoid is called martensite, which is a brittle crystalline structure.
In welding applications, martensite may form in the deposited weld metal; base material being welded; or the heat-affected zone (HAZ), which is the base metal adjacent to the fusion zone. Applying the appropriate preheat before welding will help prevent the martensite from forming. Preheat temperatures vary by the thickness, type, grade, and carbon equivalency of the base material. Note: If preheating is required, be sure to do it before any welding—including tack welding—takes place.
Second, preheating results in removing moisture (condensate) before welding. If this is not done, the moisture will change phase during welding, and hydrogen will be absorbed into the weld metal. As hydrogen diffusion has a time and temperature relationship, removing most of the moisture before welding is recommended. In short, if hydrogen molecules gets trapped in the solidified weld metal, they can wedge their way between the grain boundaries, possibly resulting in a welding failure.
Thoroughly preheating the material and covering it with an insulating medium after welding to reduce the cooling rate even more this allows the hydrogen to diffuse out of the weld joint, which prevents hydrogen cracking. Residual weld stresses and over constrained weld joints can contribute to this phenomenon as well. Sometimes you’ll need to conduct postweld stress relieving to undermine these potential issues.
About the Author
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Building a successful welding program from the ground up
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,