Independent welding consumables professional
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Consumables Corner: The right filler metal to weld duplex stainless steel
- By Nino Mascalco, Rob Koltz, and Steve Sigler
- March 16, 2015
- Article
- Consumables
Q: We manufacture stainless steel tanks used in various industries and we aren’t always informed of service conditions and chemical exposures. We would like to reduce or minimize the number of filler metals we use to cut down on costs and prevent accidental use of the wrong filler metal. The primary duplex materials we weld are 2101, 2304, and 2205 using ER2307 and ER2209 filler. Which filler metal would be best for welding these duplex base materials?
A: Yours is a common question. In general, fabricators are looking for ways to simplify the welding process and minimize the potential for costly rework or, worse, field failures of welded products. While you may already be well-versed in the fundamentals of stainless steels (SS), let's review the basics of this material group.
There are three main categories of SS in reference to its microstructure: martensitic, austenitic, and ferritic. Martensitic is outside the focus of duplex grades, so we'll leave it out of this discussion.
Austenitic SS (the 3XX series) are typically used in applications requiring good weldability. They are highly formable and offer a low-temperature service option. Ferritic SS have good strength, moderate ductility, and are relatively inexpensive.
Duplex SS (DSS) were engineered to be the best of both worlds. DSS gets its name from its metallurgical microstructure made up of approximately 50 percent austenite and 50 percent ferrite. DSS are materials that feature improved toughness and almost twice the strength of austenitic SS and feritic SS, along with improved corrosion resistance, including stress corrosion cracking (SCC).
For a pressure vessel application in which the designer/engineer has selected a specific grade of DSS and determined the required material thickness, you, the welding engineer, need to select a filler metal that is at least a matching filler metal to deliver the same properties as outlined previously. You also have the added responsibility of selecting an appropriate welding process that won’t degrade the base metal properties in the heat-affected zone (HAZ).
For example, if the job calls for a 2205 grade of DSS to be welded to itself, an ER2209 filler metal would be a solid match. However, if the base material is 2101, it’s important to realize that a lean DSS was selected because the material is less expensive than other DSS but still delivers high strength with good fatigue resistance and good corrosion resistance. The best consumable option is the matching consumable, which is ER2307, but ER2209 would be an acceptable second choice.
If the higher amount of molybdenum in the ER2209 is not a concern for the application of the finished product, it would be a fair match to weld all three of the stated DSS base materials. Because of the higher amounts of alloy in this filler metal, the cost will probably be higher.
The primary factors to consider to select the best filler metal are:
- In-service conditions such as chemical environment and temperature ranges.
- Yield and tensile strength, including whether creep resistance or high fatigue strength is required.
- Pitting resistance equivalent number (PREN) or corrosion resistance.
- Welding process and welder appeal.
- Cost.
Again, the information presented is far from exhaustive; if additional information is required, more specific details about the application of products would be needed. Additionally, many great resources are online that may be able to answer specific questions or concerns.
About the Authors
Rob Koltz
Application Engineer
411 S. Ebenezer Rd.
Florence, 29501
636-485-2253
Steve Sigler
Application Engineer
411 S. Ebenezer Rd.
Florence, South Carolina 29501
636-485-2253
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Building a successful welding program from the ground up
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,