- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Changing up the daily grind
Aluminum fabricator switches abrasives, sees immediate results
- By Amanda Carlson
- March 14, 2011
- Article
- Finishing
If it ain't broke, don't fix it, right? It's safe to say that not all change is good and that change for the sake of change seems a little unnecessary, especially if a particular system gets the job done.
But sometimes finding the ability to be open-minded toward change can result in a positive outcome. Just ask Wade Tramm, owner of Tramm Manufacturing Inc. The Isle, Minn., company manufactures marine equipment such as stainless steel railings and custom fuel cells. Its specialty, however, is fabricating custom radar arches and hard-top struts for high-profile boats, yachts, and ships.
"We do some OEM work but otherwise it's private customers. It's an elite group of people and I like working with them," Tramm explained.
Since customers turn to Tramm to help improve the appearance of their favorite pasttime—sailing their yacht—precision and quality—from initial design all the way to final aesthetics—are of the utmost importance.
In an effort to keep a close eye on quality and precision, Tramm has chosen to keep the business small, just Tramm plus three welders/fabricators.
Taming the Aluminum Beast
Fabricating and welding aluminum require specific attention to detail, particularly when it comes to surface preparation and quality.
The process starts with a picture of a customer's yacht or hull. From this Tramm formulates a design either via a CAD program or a hand-drawn sketch. After customer approval, the design is then laid out on a flat sheet of either 5052 or 6061 marine-grade aluminum. Tramm must then evaluate the best way to cut the material—by waterjet, plasma, or manually with a nibbler—based on the size and shape.
Once the material is cut, all weldable edges must be ground down to ensure surface cleanliness.
Interior components are assembled with gas metal arc welding (GMAW), and everything is tied together with gas tungsten arc welding (GTAW). GTAW provides the penetration necessary to hold the components together after the weld bead is completely ground away.
The entire fabricating process takes approximately two weeks.
No Improvement Is Too Small
Grinding is an important part of the aluminum fabrication process at Tramm. The material must be impeccably clean prior to welding to ensure final weld integrity and full bead penetration. This is especially important since 100 percent of the GTAW bead is removed before priming and painting. Improper weld penetration would result in disaster.
"To ensure that we achieve full penetration, we have to have clean material. Otherwise, if we were to grind [the weld] off, the arch would fall apart," Tramm said.
Aluminum grinding often is a messy process. At Tramm, the welders used to add wax to the 7-in. grinding wheel to help prevent the disc from filling up with aluminum dust.
"Whenever you sand aluminum, your discs fill up because the component gets hot and the material softens."
The process was messy and time-consuming, but necessary. Quite frankly, Tramm saw no reason to change.
That is until Tramm's equipment supplier introduced him to the NorZon BlueFire R884 flap disc from Norton Abrasives. The disc can perform simultaneous deburring and cleaning on aluminum.
According to Tramm, the disc gets excellent results on aluminum weld grinding because the zirconia grain microfractures, producing sharp cutting points throughout the grind. Polyester flaps help to extend disc life, and the semi-open coat gives the aluminum a place to go other than building up on the disc itself.
Once Tramm tested the Norton disc, a change started to look better.
"This new abrasive disc eliminated the need for us to use that wax, the cleaning, and the wiping down. We just immediately sand it and weld it. It saves us a lot of time, and it eliminated the need for wax 100 percent," Tramm said.
Since then Tramm has been happy with the results. The new discs have made the grinding process much faster for his welders, and it has even helped create a cleaner, more pleasant shop environment.
"The way we had been doing things had been the norm for years. It's just what we had done and it worked. I guess now with new technology we can do things differently. I'm young enough that I can be open-minded enough to try new things. By doing so I found something that works wonderfully."
Tramm Manufacturing Inc., 34994 Hwy. 47, Isle, MN 56342, 320-676-3729, www.trammarches.com
About the Author
Amanda Carlson
2135 Point Blvd
Elgin, IL 60123
815-227-8260
Amanda Carlson was named as the editor for The WELDER in January 2017. She is responsible for coordinating and writing or editing all of the magazine’s editorial content. Before joining The WELDER, Amanda was a news editor for two years, coordinating and editing all product and industry news items for several publications and thefabricator.com.
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
Three ESAB welding machines win Red Dot Awards for product design
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,