CEng
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
What welding inspectors should know about welding codes and standards
What they are, when they're used, and how they're developed
- By Tony Anderson
- January 24, 2002
- Article
- Testing and Measuring
Many aspects of welded component design and fabrication are governed by documents known as codes and standards. End users or purchasers often specify these documents in a contractual agreement to control the characteristics of the welded component that may affect its service requirements. Manufacturers also use them to assist in the development and implementation of their welding quality systems.
Many end users of welded components have developed and issued specifications that address their own requirements. However, national interest in areas such as public safety and reliability has promoted the development of welding codes and standards that command industrywide or national recognition.
For example, national engineering and technical societies have developed numerous committees that continue to evaluate the needs of industry and develop new welding codes and standards. The members of these committees are technical experts and represent all interested parties, such as manufacturers, end users, inspection authorities, and government agencies. After a committee completes a new or revised document, it usually is reviewed and approved by a review committee and published in the name of the applicable engineering society if it is accepted.
Legislative bodies or federal regulating agencies sometimes adopt documents that have significant influence on public health and safety. In those jurisdictions, such documents become law and often are referred to as codes or regulations.
Welding inspectors should know which codes and standards are applicable within their jurisdiction, understand the requirements of the relevant documents, and perform their inspections accordingly.
Sources of Welding Codes and Standards
Following are some of the more popular sources of welding codes and standards in the U.S.
American Welding Society (AWS). AWS publishes many documents addressing welding use and quality control. These documents include such general subjects as welding definitions and symbols, classification of filler metals, qualification and testing, welding processes, welding applications, and safety.
American Society of MechanicalEngineers (ASME). This society is responsible for the development of the Boiler and Pressure Vessel Code, which contains 11 sections and covers the design, construction, and inspection of boilers and pressure vessels. ASME also produces the Code for Pressure Piping, which consists of seven sections, each prescribing the minimum requirements for the design, materials, fabrication, erection, testing, and inspection of a particular type of piping system.
American Petroleum Institute (API). This institute publishes many documents relating to petroleum production, a number of which include welding requirements. The most well-known is possibly API Std 1104—Standard for Welding Pipelines and Related Facilities.
Typical Welding Code and Standard Content
The specific content and requirements of a welding code or standard can vary in detail, but they have some basic elements in common.
Scope and General Requirements. This usually is found at the beginning of the document and typically describes the type and extent of welding fabrication for which the document should be used. It also may explain limitations for the document's use.
Design. If the document provides a section for design, it may contain minimum requirements for the design of specific welded connections, or it may refer the user to a secondary source of information.
Qualification. This section typically outlines the requirements for qualification testing of welding procedure specifications, as well as the requirements for qualifying welders. It may provide the essential variables, which typically have change limitations of each variable that govern the extent of qualification. Essential variables typically include:
- The welding process
- Base metal type and thickness
- Filler metal type
- Electrical parameters
- Joint design
- Welding position
This section of the document also may provide the qualification testing requirements, which usually are divided into welding procedure and welder performance. Typically, it provides the types and sizes of test samples to be welded and prepared for testing, the testing methods to be used, and the minimum acceptance criteria to be used for evaluating the test samples.
Fabrication. This section, when included in the document, typically discusses fabrication methods or workmanship standards. It may contain information and requirements for base materials, welding consumables, shielding gas quality, and heat treatment.
Inspection. This section of the document usually addresses the welding inspector's qualification requirements and responsibilities, acceptance criteria for weld discontinuities, and the requirements for nondestructive testing procedures.
Opportunities to Improve Weld Quality and Reliability
Welding fabricators often use welding codes and standards to achieve process control to meet the requirements of ISO 9000 and other quality management systems. Often the major elements of process control specified by quality management systems are the same elements addressed in welding codes and standards:
- Production procedures must be documented. For welding, this is the welding procedure specification.
- Criteria for workmanship must be stipulated in the clearest practical manner. For welding, this may be the code or standard acceptance criteria.
- Personnel must be qualified. This may be addressed by the welder performance qualification.
Regardless of a fabricator's overall quality system, selection of the appropriate welding codes and standards can help improve welding quality and reliability even more.
About the Author
Tony Anderson
411 S. Ebenezer Road
Florence, SC 29501
800-372-2123
About the Publication
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Building a successful welding program from the ground up
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,