- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Tier 1 supplier builds four-stage competitive strategy
- By Eric Lundin
- July 24, 2003
- Article
- Hydroforming
F & P Manufacturing Inc., a Tier 1 automotive supplier, is no stranger to competitive and financial pressures. Unrelenting competitive pressures come from the many other Tier 1 suppliers looking for opportunities to increase their slice of the automotive pie. Financial pressures come from the automobile manufacturers that demand price reductions year after year.
To combat these pressures, the company examined its entire manufacturing process, which involves bending, hydroforming, and material handling.
To successfully manufacture the engine cradle for the Honda Accord®, the company set out to build the most efficient hydroforming line in North America. The company concentrated on four main areas: eliminating end scrap, decoupling the bending machines from the manufacturing line, reducing cycle time, and palletizing parts automatically.
The Part, the Plan, the Process
F & P Manufacturing, which has been involved in hydroforming since 2000, drew on its automotive metal forming experience when it developed a plan for turning a straight tube into a finished engine cradle. The part design called for a material with a tensile strength of 440 megapascals (MPa). Because the raw material had such high strength, the company paid particular attention to the material's formability to ensure that the tube wouldn't rupture during the forming process.
Hydroformed engine cradles typically are made from lengths of straight, round tube. |
A forming limit diagram (FLD) showed a few troublesome spots. The company tweaked the design by changing some of the part's design characteristics, such as corner radii. The company also incorporated a boost assist of 10,000 pounds into the bending process. As the rotary action of the bending head draws the tube into the bender, the boost assist pushes tube into the bend area. The extra tube material pushed into the bender by the boost reduces wall thinning during bending, which enhances formability for subsequent forming processes.
The hydroforming process also relies on feeding extra material. The axial feeding process, as it is called in the hydroforming industry, uses 150 tons of force. The pressure helps to reduce wall thinning as the tube expands in the hydroforming die.
Before they are hydroformed, the tubes are bent so they will fit into the hydroforming die. The benders incorporate boost assist during bending to reduce OD wall thinning. |
Eliminating Scrap."Eliminating end scrap has a big effect on efficiency," said Murray Mason, chief engineer for F & P.
A conventional hydroformed engine cradle starts out as a round tube but ends up with mostly a rectangular but varying cross section when finished. Round plugs seal the tube for the hydroforming process. After the part is hydroformed, the plugs are removed. The ends, which are round, then are cut off and discarded.
To eliminate end scrap, F & P and Schuler Hydroforming Inc., a manufacturer of metal forming equipment, collaborated to devise a process in which the entire length of tube is absorbed in the hydroforming die. The tube goes through a preforming operation that uses two dies to change the shape of the ends from round to square. Square plugs seal the tube ends for the hydroforming process, which monitors the tube end position during end feeding, and the entire tube becomes the cradle. After the tube is formed, the plugs are removed. Cutting off the ends is not necessary, so end scrap is eliminated.
Decoupling Benders. The manufacturing line was designed with flexibility so that small problems do not stop it. The line has two tube benders, which outpace the hydroforming press, and a one-hour buffer of bent tubes. The benders are decoupled for the manufacturing process so that if a problem arises with one of the benders, technicians can work on the problem while manufacturing continues.
A finished engine cradle is ready for unloading from the hydroforming die. |
Reducing Cycle Time. Reducing cycle time is critical to the success of any high-volume manufacturing operation. A complete hydroforming cycle consists of loading a part into the hydroforming press, closing the press, developing the clamping force (which keeps the die closed during hydroforming), developing the forming pressure (which shapes the part), forming the part, releasing the pressure, opening the press, and unloading the part.
"Based on our experience with manufacturing similar components and a computer simulation, we determined that a conventional hydroforming press would have had a cycle time of approximately 32 seconds for this engine cradle," Mason said.
Rather than using a conventional press, the company chose a mechanical locking press developed by Schuler. The press uses a mechanical locking feature, rather than hydraulic force, to hold the press closed during hydroforming. This eliminates the time needed to develop the clamping pressure and cuts the cycle time by 25 percent.
Palletizing Parts. A fourth operation—unloading the hydroforming press and stacking the parts—was evaluated for efficiency. This normally is accomplished manually or with an unloading system, which can be expensive, according to Mason.
The company developed its own unloading system. This approach reduced costs in two ways—it eliminated a worker and was less expensive than purchasing an off-the-shelf system.
Where Can Hydroforming Go From Here?
"This is just one step of many that are needed to push hydroforming further along in the manufacturing industry," Mason said.
"For instance, right now each hydroforming line usually is dedicated to a single part. The next step is to advance hydroforming to a point at which dies can be changed quickly and a hydroforming line can accommodate a variety of parts, similar to what we do on our stamping presses."
Such versatility, Mason said, would prevent a line from sitting idle and would thereby increase the equipment's productivity.
F & P America Manufacturing Inc., 2101 Corporate Drive, Troy, OH 45373, 937-339-0212, fax 937-339-0065, murray.mason@fandpmfg.com.Schuler Hydroforming Inc., 7145 Commerce Blvd., Canton, MI 48187, 734-207-7200, fax 734-207-7222, info@schulerinc.com, www.schulergroup.com.
About the Author
Eric Lundin
2135 Point Blvd
Elgin, IL 60123
815-227-8262
Eric Lundin worked on The Tube & Pipe Journal from 2000 to 2022.
About the Publication
Related Companies
subscribe now
The Tube and Pipe Journal became the first magazine dedicated to serving the metal tube and pipe industry in 1990. Today, it remains the only North American publication devoted to this industry, and it has become the most trusted source of information for tube and pipe professionals.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Making the move from hard automation to robotic welding
Students learn fabrication one piece at a time
Miscellaneous metals fabricator increases productivity and opportunity with plasma cutting
Get a grip on the misunderstood tube bender motor starter
Manufacturing finally sees some sunshine
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,