- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Orienting the tube’s weld seam on the mill
Seam orientation stand allows mill operators to dial in seam location
- By Eric Lundin
- November 2, 2020
- Article
- Tube and Pipe Production
Keeping the Seam on the Up-and-up
In tube production, the first area of concern for proper workpiece orientation is just before the weld box. As the two edges of the soon-to-be-welded tube come together, they form a V shape. The location of the apex of the V is critical to the welding process, especially in laser welding. The spot size of a laser is tiny, so the apex must be positioned immediately below the laser and held steady. Some laser head manufacturers assist with this, building systems that track the edges as they close in, making adjustments to the laser’s spot position as the process progresses. Still, the mill has to do the heavy lifting, keeping the strip aligned as much as possible as it feeds through each station.
Although other welding processes aren’t as exacting as laser welding, all rely on good V positioning for making reliable welds. Beyond welding, proper seam location is beneficial to scarfing the weld bead along the ID and OD, quenching the tube, and testing the integrity of the weld seam. For these processes, the location of the seam isn’t quite as critical as it is for welding, but good alignment helps.
Some other mill processes require a solid weld seam location after the weld is made. Inline seam annealing is one of them. The process relies on the same physical principle as induction welding, using a tremendous amount of electrical power to induce current flow, and therefore to develop heat, in the steel. The process anneals the weld seam and the area near the weld seam, the heat-affected zone.
“Efficient inline annealing relies on keeping the weld seam oriented with the inductors,” said Glenn Hoffmann, vice president of engineering for T & H Lemont.
Another process involves the manufacture of nonrounds formed from rounds. In some cases, the seam is supposed to be in the center of one of the sides, coinciding with the 12 o’clock location. In other cases, the seam is specified to be at some other location: a specified distance left or right of center, or a location relative to a corner or to some other tube characteristic.
Use the Mill or a Supplemental Tooling Stand
For both scenarios—keeping the seam steady at 12 o’clock or rotating it to a different specified location around the tube’s circumference—tube producers have two options. They can use specially designed rolls in place of the first sizing pass, or they can use a roll stand designed for seam orientation.
The most common way to orient the tube seam is to use rolls designed for seam orientation in the sizing section. The tools are designed with contours that impart a twisting force to direct the seam location.
The other way involves a seam orientation stand. Similar in appearance to a side-roll stand, it uses tools that can be adjusted so the shafts are slightly off vertical. The oblique angle provides a twisting force that causes the tube to rotate. Minute adjustments provide enough rotation to direct the seam to any location along the circumference between 10 o’clock and 2 o’clock.
The former method, which uses football-shaped rolls, is the less expensive of the two and is adequate for many applications, but it has a few drawbacks.
“Football-shaped rolls contact the tube over a very small surface area, so the amount of control is limited,” said Warren Wheatman, vice president of T & H Lemont’s Tooling Business Unit. Consistency and accuracy vary, Wheatman added.
Second, depending on the mill design and the tube’s characteristics, the former method might not be enough; the operator might try to get the mill to apply too much twisting force over too little distance. As with every forming and sizing process that takes place on a tube mill, finesse trumps brute force every time. Brute force often works, but wrinkles and defects are more likely to develop.
“Using a separate stand, one designed with all of the other forming parameters in mind, gives the operator more room to work, rotating the tube over a long column,” Hoffmann said. Twisting it gradually over an extended distance is preferred to applying the force abruptly in a very short space.
Another benefit to a seam orientation stand is that, for a given nonround size, just one tooling set is necessary. For example, if a tube maker makes quite a bit of 2-in. square tubing with the weld seams specified in a variety of locations, a single tooling set can cover all of its orders of 2-in. square product.
Manually Adjusted or Remote-controlled
Some seam orientation stands are designed and built to have two adjustments, and some have three. The primary adjustments are lateral roll position to accommodate various tube sizes and tooling offset to determine the amount of twist. A third is vertical roll position so the stand can adapt to varying passline heights.
The two main varieties of seam orientation stand are manual and remote-controlled. Regardless of whether the stand is manually or remotely controlled, the tooling positions and the amount of offset normally are set before threading the strip through the mill.
“The big advantage of remote control is in the amount of uptime,” said Jim Godzicki, lead mill service technician. “When using the remote control, the operator can adjust the amount of twist on the fly without shutting down the mill.”
About the Author
Eric Lundin
2135 Point Blvd
Elgin, IL 60123
815-227-8262
Eric Lundin worked on The Tube & Pipe Journal from 2000 to 2022.
About the Publication
subscribe now
The Tube and Pipe Journal became the first magazine dedicated to serving the metal tube and pipe industry in 1990. Today, it remains the only North American publication devoted to this industry, and it has become the most trusted source of information for tube and pipe professionals.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Making the move from hard automation to robotic welding
Students learn fabrication one piece at a time
Miscellaneous metals fabricator increases productivity and opportunity with plasma cutting
Get a grip on the misunderstood tube bender motor starter
Manufacturing finally sees some sunshine
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,