Contributing Writer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Dean C. Phillips
Hobart Brothers Co.
101 Trade Square
Troy, OH 45373
937-332-4000
- From The Fabricator
Welding metals of dissimilar strengths
- By Dean C. Phillips
- Apr 30, 2010
- Arc Welding
- Article
Welding metals of dissimilar strengths requires that a welder consider some specific factors, to ensure a solid joint.
- From The Fabricator
Welding ASTM A514 or A514M-05 steel?
- By Dean C. Phillips
- Jun 12, 2007
- Arc Welding
- Article
As manufacturers strive for lower costs and greater efficiencies, they tend to substitute high-strength materials for standard materials. One such high-strength material is ASTM A514/514M-05. Although it is not difficult to weld, joining it successfully requires paying close attention to the preheat temperature, interpass temperature, and filler metal.
- From The Fabricator
Implementing Press Automation
- By Dean C. Phillips
- Jun 13, 2006
- Bending and Forming
- Article
By mixing press automation with electronic controls, job shops can increase output and exceed manufacturing goals. Learn about press automation from FMA's experts.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1
Managing Dangerous Dusts from Metalworking
- June 26, 2024
- Sponsored
- Presented By: Camfil Air Pollution Control