President
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Dr. Yehuda Baskin
Superior Flux & Manufacturing Co.
6615 Parkland Blvd.
Cleveland, OH 44139
440-339-3000
- From The Welder
Detailing DeepTIG
- By Dr. Ian Harris, Dr. Yehuda Baskin, and Philip A. Baskin
- Jul 28, 2017
- Arc Welding
- Article
EWI DeepTIG uses specialized metal oxides to increase weld penetration in GTAW. The patented process uses proprietary oxide formulations which, when applied to the surface of the workpieces to be joined, increases weld penetration and consequently enhances process productivity. It has been shown to increase weld penetration in GTAW by up to 300 percent.
Improving 400 series weld seams in tube, pipe production
- By Cary B. Long and Dr. Yehuda Baskin
- Feb 3, 2016
- Tube and Pipe Fabrication
- Article
Chromium is a miracle element when added to iron, combining with oxygen to form chromium oxide, the compound that prevents rust in stainless steels. The downside is that it also impedes bonding, making stainless difficult to weld. Using a flux can help by improving weld quality and allowing faster welding speeds.
Improving GTAW for producers, fabricators
- By Dr. Yehuda Baskin and Dr. Ian Harris
- Jul 19, 2013
- Arc Welding
- Article
Gas tungsten arc welding, a joining process developed decades ago, has been improved by many technology developments over the years, but the essentials are unchanged: It uses an electric arc between a nonconsumable tungsten electrode and the workpiece to produce a weld pool, and it uses a shielding gas. Experiments with brushing on or pasting on mixed metal oxide slurries have shown how this decades-old process can improve dramatically in penetration and speed.
Looking to improve weld seams?
- By Dr. Yehuda Baskin
- Sep 1, 2009
- Tube and Pipe Production
- Article
Most tube and pipe producers weld the seam as it is—without additives or fillers—and risk the problems associated with oxidation. A specially formulated brazing flux, in liquid or paste form, dissolves and removes oxides, prevents re-oxidation, and helps transfer weld heat to the seam.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1
Managing Dangerous Dusts from Metalworking
- June 26, 2024
- Sponsored
- Presented By: Camfil Air Pollution Control