Orbital Welding Machine Buyers' Guide



 
OD Range
Type
Process
Torch Rating
Features
Power Supply
Model/Series Inches Millimeters Other Amps Model

Arc Machines Inc.  Pacoima, CA

6 .125 - 1.500 3.2 - 38.1 200 100 0 E W 227/415 Varies 200/400 100
8 Series .25-6.625 6.3-169 200 W 205/207/307/217 WDR 100/240/1 150 100
9 Series .250-7.500 6.3-190.5 200 W 205/207/307/217 WDR 100/240/1 150 100
9-250 .093-.250 2.3-6.3 50 G 205/207/307/217 WDR 110/240/1 150 100
9-500/9-500C .093-.500 2.3-12.7 75 G 205/207/307/217 WDR 240/1 150 100
9-675/750 .093-.750 2.3-19 200 W 205/207/307/217 WDR 100/240/1 150 100
15 3.500 - Inf. 88.9 - Inf. 300 100 0 E W 415/227 Varies 200/400 100
43 6.75-24.0 ID 171-610 ID 250 100 0 E W 415/501 Any 3 ø 400 100
44 2-31.5 51-800 300 100 0 W 415 Any 3ø 400 100
52 NGT 8.625-Inf. 219-Inf. 300 100 0 E W 415/501 Any 3 ø 400 100
62 8.625 219 300 100 0 E W 415/501 Any 3ø 400 100
73 5.16-20.0 ID 131-508 ID 250 100 0 E W 227/415 Varies 200/400 100
79 Series .75-6.625 19-170 200 100 0 E W 227/415 Varies 200/400 100
81 1.900-5.567 48-142 200 100 0 E W 227/415 Varies 200/400 100
85 .375-.75 9.5-1.9 100 100 0 M W 205/207/227/307 Varies 150/200 100
88 .875-3.0 22-203 200 100 0 E W 327/415 Varies 250/400 100
94 .68-6.75 ID 17-171 ID 250 100 0 E W 227/415 Varies 200/400 100
95 Series .750-6.625 19-170 250 100 0 M W 227/307/415 Varies 150/400 100
96 .375-1.87 ID 9.525-47.5 ID 150 100 E W 205/207/307/227/415/217 WDR Varies 150/400 100
RDE-005 Rotor Driver .125-2.000 3.2-38.1 75 G 205/207/307 100/240/1 150 100

Axxair  Alvin, TX

SAFT-40ND .25 - 1.5 6 - 40 110 100 X W SASL-161T 115/26/1 110 100
SATF-40MI .25 - 1.5 6 - 40 120 100 W Compatible with AMI 205/207
SATF-65ND .25 - 2.5 6 - 65 110 100 X W SASL-161T 115/26/1 110 100
SATF-65MI .25 - 2.5 6 - 65 120 100 W Compatible with AMI 205/207
SATF-115ND 1 - 4.5 25.4 - 115 110 100 X W SASL-161T 115/26/1 110 100
SATF-115MI 1 - 4.5 25.4 - 115 120 100 W Compatible with AMI 205/207

Magnatech LLC  East Granby, CT

428A 1.315-3.5 33-88.9 200 100 M W 514, 515, 516 230/30/1 200 100
429A 3.5-6.625 89-168.3 200 100 M W 514, 515, 516 230/30/1 200 100
432 1.0-3.5 25-88.9 200 100 E W 515, 516 230/480/15/1 or 3 200/600 100
433 2.375-6.625 60-168.3 200 100 E W 515, 516 230/480/15/1 or 3 200/600 100
420 1.0-6.625 25.4-168.3 200 100 E W 515, 516 230/480/15/1 or 3 200/600 100
419 6.625-60.0 168-1,524 300 100 E W 515, 516 230/480/15/1 or 3 600 100
419 Narrow Gap 6.625-60.0 168-1,524 500 100 E W 515, 516 230/480/15/1 or 3 600 100
Pipeliner II 6.625-60 168-1,524 GMAW, FCAW 300 100 E W MS4000 230/480/15/3 400 100
M-500 .125"-.500" 3-12.7 75 100 G 514 230/30/1
805 .125-.625 3-16 100 100 W 514, 515, 516 230/30/1 200 100
810 .125-1.0 3-25.4 120 60 W 514, 515, 516 230/30/1 200 100
820 .25-2.0 6-50.8 120 60 W 514, 515, 516 230/30/1 200 100
830 .375-3.0 9-76.2 120 60 W 514, 515, 516 230/30/1 200 100
840 .5-4.0 12-104 120 60 W 514, 515, 516 230/30/1 200 100
860 2.0-6.0 50.4-168.3 120 60 514, 515, 516 230/30/1 200 100
427A .5-1.5 13-38.1 200 100 M W 514, 515, 516 230/30/1 200 100

Otto Arc Systems, Inc.  El Dorado Hills, CA

 TPWH-C  .125-6.625  3-168         W
 OW-ARC-180        180      W OW-ARC-180  230 180 180@35
 OW-ARC-250        250     W  OW-ARC-250 220 250 250@60
 OW-ARC-450        450  300@70   W  OW-ARC-450 480  400  400@60
 TPWH-O  .625-5  15.88-127        E  W        
 TPWH-OA  .75-12 19.05-304.8       E W        
 TPWH-NS-2 1.26- 2 32-51          W        
 PWH-LD 8-34 203.2-863.60       E W        
 TSWH-1.5 .63-1.5  16-38  Tube Sheet Weld Head Fusion  180  100@70  E W        
 TSWH .375-3.15  8-80  Tube Sheet Weld Head Wire & Fusion  450  300@70  E  W        
 TSWH-HB 1-1.25  25-32 Tube Sheet- Header Box Welding  400  200@60  E W        

Tri Tool Inc.  Rancho Cordova, CA

AdaptArc(R) and OrbitMaster(R) 2.375-Inf. 171-Inf. GMAW-S, GMAW-P, FCAW 340 100 E W Miller XMT or Big Blue Series 208-575/1 or 3 450 100