44
Specifications
Model/Series | 44 |
OD Range - Inches | 2-31.5 |
OD Range - Millimeters | 51-800 |
Type - Closed Chamber-Electrode Enclosed | |
Type - Open Head Exposed Torch | |
Type - Carriage Welding Head-Exposed Torch | |
Process - GTAW | |
Process - Other | |
Torch Rating - Amps | 300 |
Torch Rating - Duty Cycle (percent) | 100 |
Torch Rating - Pulsed | 0 |
Features - Arc Length Control (E = Electronic, M = Mechanical) | |
Features - Filler Wire | |
Features - Cooling (G = Gas, W = Water) | W |
Features - Multipass Capacity For Groove Welds | |
Power Supply - Model | 415 |
Power Supply - Maximum Input (volts/amps/phase) | Any 3ø |
Power Supply - Maximum Output (Amps) | 400 |
Power Supply - Duty Cycle (Percent) | 100 |
Arc Machines Inc.
10500 Orbital Way
Pacoima, CA 91331
Phone: 818-896-9556
Fax: 818-890-3724
arcmachines.com
10500 Orbital Way
Pacoima, CA 91331
Phone: 818-896-9556
Fax: 818-890-3724
arcmachines.com