Bystronic Inc.  Elgin, IL

ByJet Flex 1530 252 280 120 60 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct  25 52 .66
ByJet Flex 1530 252 280 120 60 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52  1.32
ByJet Flex 1530 252 280 120 60 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 1530 252 280 120 60 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra + 124 77 1.45
ByJet Flex 2030 280 280 120 82 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct 25 52 .66
ByJet Flex 2030 280 280 120 82 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52 1.32
ByJet Flex 2030 280 280 120 82 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 2030  280 280  120  82 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra +  124  77  1.45
ByJet Flex 4030 359 280 160 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct 25 52 .66
ByJet Flex 4030 359 280 160 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52 1.32
ByJet Flex 4030 359 280 160 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 4030 359 280 160 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra + 124 77 1.45
ByJet Flex 6030 437 280 239 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct 25 52 .66
ByJet Flex 6030 437 280 239 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52 1.32
ByJet Flex 6030 437 280 239 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 6030 437 280 239 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra + 124 77 1.45
ByJet Flex 8030 516 280 318 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct 25 52 .66
ByJet Flex 8030 516 280 318 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52 1.32
ByJet Flex 8030 516 280 318 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 8030 516 280 318 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra + 124 77 1.45
ByJet Flex 10030 595 280 397 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct 25 52 .66
ByJet Flex 10030 595 280 397 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Direct + 50 52 1.32
ByJet Flex 10030 595 280 397 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra 60 77 .66
ByJet Flex 10030 595 280 397 120 9.84 .002 .001 4 A DXF, DWG, MI, IGES, STEP Bystronic ByPump Ultra + 124 77 1.45

ESAB Welding & Cutting Products  Florence, SC

Hydrocut LX 216 - 888 183 - 301 672 220 8 .01 .002 3 A DWG, DXF KMT HP Intensifier 200 90 1.43

Hypertherm Inc.  Hanover, NH

HyPrecision™ 15 70 34 Hypertherm HyPrecision™ 15 15 60 .3
HyPrecision™ 30 70 34 Hypertherm HyPrecision™ 30 30 60 .6
HyPrecision™ 50 70 34 Hypertherm HyPrecision™ 50 50 60 1.0
HyPrecision™ 50S 76 40 Hypertherm HyPrecision™ 50S 50 60 1.1
HyPrecision™ 60S 76 40 Hypertherm HyPrecision™ 60S 60 60 1.3
HyPrecision™ 75S 76 40 Hypertherm HyPrecision™ 75S 75 60 1.6
HyPrecision™ 100D 86 45 Hypertherm HyPrecision™ 100D 100 60 2.2
HyPrecision™ 150D 81 55 Hypertherm HyPrecision™ 150D 150 60 3.2

Flow Waterjet  Kent, WA

Mach 2 1313b 107 81 50 50 8 .005 .002 3 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 2 2031b 163 158 78 120 8 .005 .0025 3 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 2 4020b 163 193 157 78 8 .005 .0025 3 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 2 2020c 130 122 78 78 6 .005 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 2 2030c 173 122 78 122 6 .005 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 2 2040c 212 122 79 157 6 .005 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 100 60 2
Mach 3 1313b 142 101 50 50 8 .0015 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 3 2513b 150 151 98 50 8 .0015 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 3 3020b 178 170 122 78 8 .0015 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 3 4020b 178 212 157 78 8 .0015 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 3 7320b 178 381 288 78 8 .0015 .002 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 2020c 155 199 78 78 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 2080c 199 413 78 314 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 3020c 155 239 120 78 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 3030c 196 239 120 120 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 3080c 413 239 120 314 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 30100c 498 239 120 393 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 30130c 628 239 120 511 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 4020c 155 278 157 78 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 4030c 196 278 157 120 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 4050c 284 278 157 196 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 4070c 369 278 157 275 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 40100c 498 278 157 393 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 40110c 543 278 157 433 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4
Mach 4 40140c 672 278 157 550 12 .001 .001 5 A AI, D, I, DWG, SLDPRT, Step, Catia, ORD Flow Intl. Direct drive, Intensifier 200 94 4

Hydrapower Intl. Inc.  Marco Island, FL

SQ3020 120 80 .004 .004 .004 .004 .002 3 A AI D IGES KMT UHP 50 60 1

International Waterjet Machines  Alhambra, CA

 WC5WA2513H      96/.0008/.0004 48/.0008/.0004  6      3 A DXF, G-code  IWM USA WIP5 50 55 .8
 WC5WA3216H      120  60  6     3 A DXF, G-code IWM USA WIP5 50 55 .8
 WC5WA3020H      120  79 6      3 A DXF, G-code IWM USA WIP5 50 55 .8
 WC5WA6030H     120  61.75 6     3 A DXF, G-code IWM USA WIP5 50 55 .8
 WC5WA1313H      48/.0008/.0004   48/.0008/.0004  6      3  DXF, G-code  IWM USA  WIP5  50  55  .8

Jet Edge  St. Michael, MN

MR55 60 60 12 12 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR58 60 96 96 60 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR513 60 156 156 60 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR85 96 60 60 96 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR813 96 156 156 96 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR1313 156 156 156 156 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR2113 252 156 156 252 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
MR2413 252 156 156 252 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR44 48 48 48 48 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR48 48 96 96 48 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR412 48 144 144 48 12 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR68 72 96 96 72 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR610 72 120 120 72 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR612 72 144 144 72 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR614 72 168 168 72 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR84 96 48 48 96 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR812 96 144 144 96 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR814 96 168 168 96 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR1012 120 144 144 120 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR1014 120 168 168 120 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR128 144 96 96 144 12/18 .001 .001 3/5 A Ai, D, I Jet Edge iP, xP Series 200 90 4
HR1212 144 144 144 144 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR1214 144 168 168 144 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR148 168 96 96 168 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR1414 168 168 168 168 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR168 192 96 96 192 12/18 .001 .001 3/5 A Ai, D, I Jet Edge iP, xP Series 200 90 4
HR1610 192 120 120 192 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4
HR1812 216 144 144 216 12/18 .001 .001 3/5 A Ai, D, I Jet Edge iP, xP Series 200 90 4
HR2410 240 120 120 240 12/18 .001 .001 3/5 A AI, D, I Jet Edge iP, xP Series 200 90 4

KMT Waterjet Systems  Baxter Springs, KS

View Details KMT Streamline PRO2 125 125 90 1.43
View Details KMT Streamline PRO2 60 60 90 .73
View Details KMT Streamline SL-V 50 50 60 1.0
View Details KMT Streamline SL-V 100 100 60 2.0
View Details KMT Streamline SL-V 200 200 60 4.0
View Details KMT SL-V 15Plus 15 60 .30
View Details KMT Streamline S30 30 60 .52
View Details KMT Streamline S50 50 60 .88
View Details KMT Streamline E30 30 55 .6
View Details KMT Streamline E50 50 55 1.0
View Details KMT NEOLine 40 55 .72

KNUTH Machine Tools USA Inc.  Lincolnshire, IL

Hydro-Jet Eco 0515 SL 102 161 59 19.7 3 .0012 .0012 2 A D, DIN/ISO BFT 38.37 50 55 1
Hydro-Jet Vario 1313 114 110 51 51 6 .004 .002 3 A D, DIN/ISO BFT 38.37 50 55 1
Hydro-Jet Vario 1525 146 146 98 59 6 .004 .002 3 A D, DIN/ISO BFT 38.37 50 55 1
Hydro-Jet Vario 1530 146 165 118 59 6 .004 .002 3 A D, DIN/ISO BFT 38.37 50 55 1
Hydro-Jet Vario 2040 165 205 157 79 6 .004 .002 3 A D, DIN/ISO BFT 38.37 50 55 1
Stahlwerk Premium 3015 177 90 120 61 8 .0012 .0008 3 A D, DIN/ISO BFT 38.37 50 55 1
Stahlwerk Premium 3020 177 90 120 81 8 .0012 .0008 3 A D, DIN/ISO BFT 38.37 50 55 1
 Stahlwerk Premium 3065 177 319 120 258 8 .002 .0012 3 A D, DIN/ISO BFT 38.37 50 55 1
 Stahlwerk Premium 3080 177 378  120  317  8 .002 .0012  3 A  D, DIN/ISO  BFT  38.37  50  55  1
 Stahlwerk Premium 4020 216 110 159 81 8 .0012 .0008 3 A D, DIN/ISO  BFT 38.37 50 55 1
 Stahlwerk Premium 4030 216 153 159 120 8 .0012 .0008 3 A D, DIN/ISO BFT 38.37 50 55 1

Koike Aronson Inc.  Arcade, NY

 K-Jet 184 112 12  6  12  .005  .002  Flashcut CNC - 3 M  DXF, DWG  Hypertherm  HyPrecision 60  60  3.5
K-Jet Pro 184 112 12 6 12 .005 .002  Hypertherm Edge Connect - 3 M  DXF, DWG  Hypertherm HyPrecision   150 60 4

OMAX  Kent, WA

OMAX 2626 116 72 29 26 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 2652 139 67 52 26 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 5555 131 95 55 55 8 .001 .001 5 A All OMAX EnduroMAX 100 60 2.25
OMAX 55100 155 94 100 55 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 60120 225 110 126 62 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 80X 265 152 160 80 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 80X-1 338 154 240 82 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 80X-2 420 180 321 82 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 120X/S 261 207 160 120 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 120X 340 207 240 120 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 120X-1 420 230 321 120 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 120X-2 501 230 400 120 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 120X-3 586 230 480 120 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 160X 420 271 322 161 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 160X-1 502 271 400 160 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 160X-2 586 271 480 160 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX 160X-3 660 271 561 160 8 .001 .001 6 A All OMAX EnduroMAX 100 60 2.25
OMAX MicroMAX 68 70 24 24 4 .0006 .0001 6 A All OMAX EnduroMAX 30 60 .72
MAXIEM 0707 80 99 32 31 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, Raster OMAX Direct Drive 40 50 1.09
MAXIEM 1515 111 121 62 62 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09
MAXIEM 1530 169 121 120 62 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09
MAXIEM 2030 169 146 120 80 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09
MAXIEM 2040 216 146 157 80 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, Raster OMAX Direct Drive 40 50 1.09
MAXIEM 2060 295 146 247 80 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09
MAXIEM 2080 375 146 326 80 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09
MAXIEM 3060 295 190 247 122 12 .003 .001 5 A DWG, DXF, OMX, ORD, AI, PDF, SVG, RASTER OMAX Direct Drive 40 50 1.09

PaR Systems Inc.  Shoreview, MN

Vector To spec. To spec. To spec. To spec. To spec. 5 A To spec. KMT 100,000

Semyx LLC  Dalton, GA

 Phantom 324  189 160  120  95  7  .001  .0002  3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Phantom 424 236 160  158 95 7 .001 .0002 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Infinity 340 248 177 120 160 7 .002 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
Infinity 360 366 177 120 240 7 .002 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Infinity 380 425 177 120 315 7 .002 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Infinity 3120 661 177 120 472  7 .002 .002  3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Infinity 460  366 216 160 240 7 .002 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
Infinity 480 425 216 160 315 7 .002 .001  3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Infinity 4120 661 216 160 472 7 .002 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Cobra 240 195.7 132.3 160 78 7 .0078 .002 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Cobra 590 248.25 415.5 360 180 4.5 .008 .002 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Cobra 5100 248.25 451.5 396 180 4.5 .008 .002 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Cobra 5120 248.25 535.5 480 180 4.5 .008 .002 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
Optima 260 268 132 80 240 7 .004 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Optima 320 111 178 120 78 7 .004 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Optima 420  111 222.5 160 78 7 .004 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Scorpion 316 159 141 120 63 7 .003 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Genesis s12 106 79 47 47 7 .004 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    
 Genesis s16 123 95 63 63 7 .004 .001 3 M AI, CDR, CGM, DXF, DWG, EMF, EPS, FH, PIC, PCT, SWT, SVG, WMF BFT 50    

TECHNI Waterjet  Lenexa, KS

Intec-G2 i510 168 92 120 60 8 .005 .001 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
Intec-G2 i612 192 102 144 72 8 .006 .002 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
TJ3000-X3 168 92 120 60 8 .001 .0005 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
TJ4000-X3 192 102 144 72 8 .001 .0005 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
TJ5000-X3 166 236 180 120 8 .001 .0005 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
TJ6000-X3 166 315 240 120 8 .001 .0005 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
TJ4100-G 94 173 156 84 8 .001 .0005 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
Intec-G2 i1015 166 236 180 120 8 .006 .002 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
Intec-G2 i1020 166 315 240 120 8 .006 .002 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8
Intec-G2 i713 94 173 156 84 8 .006 .002 3/5 A DXF Techni Waterjet Quantum NXT 66 66 .8

WARDJet Inc.  Tallmadge, OH

 WARDKit 2x2 59 59 25 25 12 .003 .001 8 A AI, D, I Hypertherm  HyPrecision 150 60  3.2
 WARDKit 5x5 108 90 60 60 12 .003 .001 8 A AI, D, I Hypertherm  HyPrecision 150 60 3.2
 WARDKit 5x10 180 90 120 60 12 .003  .001 8 A AI, D, I Hypertherm  HyPrecision 150 60 3.2
 E-0606 59 59 25 25 12 .003 .001 8 A AI, D, I Hypertherm  HyPrecision 150 60  3.2
E-1515 108 90 60 60 12 .003 .001 8 A AI, D, I Hypertherm HyPrecision 150 60 3.2
E-1530 180 90 120 60 12 .003 .001 8 A AI, D, I Hypertherm HyPrecision 150 60 3.2
 E-2040  214  113 157  79  12  .003  .001  8 A  AI, D, I  Hypertherm HyPrecision  150  60  3.2
Custom Any Any To spec. To spec. To spec. .003 .001 32 A AI, D, I Hypertherm HyPrecision 150 60 3.2
G-4018 655 256 480 216 60 .003 .001 32 A AI, D, I Hypertherm HyPrecision 150 60 3.2
G-6018 900 256 720 216 60 .003 .001 32 A AI, D, I Hypertherm HyPrecision 150 60 3.2
J-138 118 195 97 147 12 .006 .002 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
L-1212 239 239 145 147 12 .003 .001 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
R-1214 240 250 145 157 12 .003 .001 16 A D, AI, I Hypertherm HyPrecision 150 60 3.2
R-2014 360 250 241 157 12 .003 .001 16 A D, AI, I Hypertherm HyPrecision 150 60 3.2
R-2014-36 360 250 241 157 36 .003 .001 16 A D, I, AI Hypertherm HyPrecision 150 60 3.2
R-3014 480 250 361 157 12 .003 .001 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
 R-3014-36 480  250 361 157 36 .003 .001 16 A  AI, D, I  Hypertherm  Hypertherm 150 60 3.2
R-4014 600 250 481 157 12 .003 .001 16 A D, AI, I Hypertherm HyPrecision 150 60 3.2
 R-4014-36 600 250 481 157 36 .003 .001 16 A  AI, D, I  Hypertherm  Hypertherm  150  60  3.2
 R-5014 750 250 600 157 12 .003 .001 16 A AI, D, I Hypertherm  HyPrecision 150 60 3.2
 R-5014-36  750 250 600 157 36 .003  .001  8 A  AI, D, I  Hypertherm  Hypertherm  150  60  3.2
 Z-1530-36 201  121  120 60 36 .003 .001 16 A  AI, D, I  Hypertherm  Hypertherm  150  60  3.2
Z-2043 225 110 156 78 12 .003 .001 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
Z-2543 225 132 156 97 12 .003 .001 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
Z-2543-36 225 147 156 97 36 .003 .001 16 A AI, D, I Hypertherm HyPrecision 150 60 3.2
 Z-3043 225 167 156 120 12 .003 .001 16 A AI, D, I Hypertherm  HyPrecision 150 60 3.2
 Z-3064  315 156 120 252 12 .003 .001 16 A AI, D, I Hypertherm  HyPrecision 150 60  3.2