Contributing Writer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Choosing the proper steel to minimize abrasive adhesive tool wear
- By Thomas Hillskog
- September 25, 2003
- Article
- Bending and Forming
Many tools crack because of abrasive or adhesive wear. If one type is mistaken for the other, the actions taken to extend the life of a tool can have the opposite effect.
Abrasive Wear
Abrasive wear is caused by hard particles, such as carbides and inclusions, on the surface or within the work material. These particles act as microcutting tools on a microscopic scale.
Figure 1 High magnification of a punch edge shows a characteristic pattern caused by abrasive wear. |
Because of the motion between the punch and work material, small microchips are cut out of the tool, which leads to a gradual loss of tooling material. On a macroscopic level, this type of tool wear causes a rounding of the punch edge, yet the punch still appears relatively smooth (see Figure 1). A closer inspection shows characteristic parallel scratch marks on the edge and along the sides of a punch where particles cut into the tool surface during the stamping.
The following actions might help to improve abrasive wear resistance:
• Increase steel matrix hardness. This can be achieved by increasing the hardening temperature or adjusting the steel's tempering temperature.
• Use steel that contains a high percentage of hard carbides. D2 and M2 are examples of traditional steels that contain carbides to improve wear resistance. Because of conventional production methods, the carbides in these steels are large and nonuniformly distributed.
This means that when cutting particles that are embedded in the work material move across the tool surface, they encounter fewer carbides, and a large portion of the softer steel matrix is exposed to their cutting action. The chemistry of traditional carbide steels was designed years ago, and the carbides are relatively soft with a Vicker's hardness of approximately 1,700.
• Change to powder metallurgical (P/M) produced steels that are designed to offer a higher degree of abrasive wear resistance. The P/M manufacturing process creates smaller, uniformly distributed carbides in the steel matrix and allows for the use of different alloying elements. This results in a harder carbide with a Vicker's hardness of approximately 2,800. Cutting particles encounter more and harder carbides as they move across the tool surface, and P/M steel can offer a better protection of the steel matrix.
For example, P/M M4 is a common grade for high-end cold-work applications if a high hardness for compressive strength and good abrasive wear resistance are needed. However, M4 is based on older chemistry, and new P/M grades have been developed specifically for cold-work applications. These newer materials are designed to have a better balance of cracking or chipping resistance and good wear properties.
P/M steels normally give the best protection for against abrasive wear of a tool surface. However, in some situations conventional steels with their large, blocky carbides are more cost-effective, such as if the cutting particles in the work material are much larger than the carbides in the P/M steel.
The microchips formed by the abrasive particles are so thick that they remove the smaller P/M carbides together with the matrix. The blocky carbides of conventionally produced steels like D2, D3, or D6 are larger than the abrasive particles' depth of cut and protect the softer steel matrix better than P/M steels in this case. For example, D3 or D6 often is used in brick pressing because the work material consists of refractory particles, which are very hard and larger than P/M steel carbides. Increasing the hardness and using highly alloyed P/M steels can improve performance in applications like brick pressing. However, the price-to-performance ratio normally is insufficient to use P/M steels for these applications.
• Tungsten carbide has a high volume of evenly distributed small and hard carbides to resist abrasive wear. The limitations of this tooling material are its lack of toughness, which can lead to cracking or chipping, combined with high initial toolmaking costs.
When the correct tooling material is found for the application, which creates stable working conditions without chipping or cracking, a surface coating can further improve the tool's abrasive wear resistance.
Adhesive Wear
Adhesive tool wear occurs when soft, adhesive work materials, such as aluminum, copper, stainless steels, and low-carbon steels, are used. Conditions that increase adhesive wear are high friction and heavy loading.
The origin of adhesive wear is the formation of microwelds between localized contact points on the tool and work material surface. During the movement of the tool and work material, these microwelds are broken up. If breakage takes place in the tool surface, small fragments will be torn out, which leads to a gradual loss of material.
Figure 2 On a macroscopic scale, adhesive wear can cause microcracks, which will lead to an uneven appearance of the tool's edge. |
Even if the microwelds do not break in the tool surface, repeated tearing will lead to the formation of microcracks. Over time these cracks will grow together, and when they reach a critical size, larger pieces of the edge will start to break out. On a macroscopic scale, adhesive wear leads to an uneven appearance of the tool's edge (see Figure 2) compared to abrasive wear, in which pieces are torn out of the tool surface.
To reduce adhesive wear, consider the following tool steel properties:
• Low coefficient of friction. This requires a good tool surface finish, preferably with the grinding and polishing performed parallel with the direction of tooling movement. Other solutions include lubricants or surface coatings.
• High yield strength. This creates a better resistance to breakage of tool surface microwelds and the forming of microcracks because of the repeated tearing action.
• Hard carbides in the matrix. Microwelds cannot form between the carbides and the work material; therefore, a high carbide volume in the tool steel will reduce adhesive wear. However, a small carbide size and even distribution are important because of their detrimental effect on tool steel ductility.
• High ductility. High ductility means that the tool steel can deform on a microscopic scale rather than forming cracks and therefore resist breakage or chipping. Cold work grades like D2, D3, and M2 have a low adhesive wear resistance because of their large, blocky, nonuniform carbide distribution. This microstructure results in tool steel with low ductility. Low ductility in these steel types can cause microweld breakage in the tool rather than in the work material, and it also leads to a rapid formation and growth of microcracks, which will result in chipping of tool edges.
The smaller size and uniform distribution of the carbides in the matrix of P/M steels produce a higher ductility than in conventionally produced steels with similar carbide volume and hardness. P/M steels have a better resistance to microweld formation, breakage of the welds in the tool surface, and the formation of microcracks that lead to chipping.
Because ductility is an important property for good adhesive wear resistance, anything that compromises tool ductility should be minimized for optimum tool life. The limiting factor for ductility in P/M steel is internal defects, mainly the nonmetallic inclusion content.
During the last decade P/M steel producers have developed new grades with reduced content of internal defects. These second- and third-generation P/M tool steels are designed to have higher ductility than standard P/M grades with similar alloying content, which improves their adhesive wear resistance.
Distinguishing Wear Types
An increase in matrix hardness and volume of hard, uniformly distributed carbides in tooling material can improve its abrasive wear resistance. High ductility combined with well-distributed, small carbides increase adhesive wear resistance.
However, high matrix hardness and carbide volume, necessary for good abrasive wear resistance, also lead to lower ductility and decreased adhesive wear resistance. This contradiction is why it's important to establish which type of wear is dominating an application before taking actions to correct the problem.
Thomas Hillskog is a technical manager for Bohler-Uddeholm Corp., 4902 Tollview Drive, Rolling Meadows, IL 60008-3729, 847-577-2220, fax 847-577-8028, www.bohleruddeholm.com.
About the Author
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Washington artist creates life-size elk sculptures
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,